| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.53 g/cc | 0.0553 lb/in³ | ISO 1183 |
| Water Absorption | 0.20 % @Temperature 23.0 °C |
0.20 % @Temperature 73.4 °F |
RMC 93%; DIN EN ISO 62 |
| Moisture Absorption at Equilibrium | 0.40 % | 0.40 % | DIN EN ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | >= 100 | >= 100 | DIN 53505 |
| Hardness, Shore D | 90 | 90 | DIN 53505 |
| Ball Indentation Hardness | 160 MPa | 23200 psi | DIN 2039 |
| Tensile Strength at Break | 93.1 MPa | 13500 psi | DIN EN ISO 527 |
| Tensile Strength | 93.1 MPa | 13500 psi | DIN EN ISO 527 |
| Tensile Stress | 44.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
6380 psi @Strain 1.00 %, Time 1000 hour |
DIN 53444 |
| Tensile Strength, Yield | 61.0 MPa | 8850 psi | Elastic Limit |
| Elongation at Break | 6.8 % | 6.8 % | Flexural; DIN EN ISO 178 |
| 6.8 % | 6.8 % | DIN EN ISO 527 | |
| Elongation at Yield | 2.4 % | 2.4 % | Elastic Yield Point |
| 4.3 % | 4.3 % | Flexural; DIN EN ISO 178 | |
| 6.8 % | 6.8 % | Elongation at Maximum Force; DIN EN ISO 527 | |
| Tensile Modulus | 2.48 GPa | 360 ksi | DIN EN ISO 527 |
| Flexural Strength | 177 MPa | 25700 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 |
| 182 MPa | 26400 psi | DIN EN ISO 178 | |
| 182 MPa | 26400 psi | DIN EN ISO 178 | |
| Flexural Modulus | 8.83 GPa | 1280 ksi | DIN EN ISO 178 |
| Compressive Strength | 101 MPa | 14600 psi | Elastic Limit |
| 147 MPa | 21300 psi | break; DIN EN ISO 604 | |
| 147 MPa | 21300 psi | DIN EN ISO 604 | |
| 61.0 MPa @Time 3.60e+7 sec |
8850 psi @Time 10000 hour |
||
| 95.0 MPa @Time 360000 sec |
13800 psi @Time 100 hour |
||
| 108 MPa @Time 36.0 sec |
15700 psi @Time 0.0100 hour |
||
| 83.0 MPa @Strain 3.50 % |
12000 psi @Strain 3.50 % |
DIN EN ISO 604 | |
| Compressive Modulus | 1.95 GPa | 283 ksi | DIN EN ISO 604 |
| Fatigue Strength | 55.0 MPa @# of Cycles 1.00e+6 |
7980 psi @# of Cycles 1.00e+6 |
1 Hz |
| K Factor (ISO) | 0.10 µm/km @Temperature 20.0 °C |
0.10 µm/km @Temperature 68.0 °F |
|
| 0.70 µm/km @Temperature 100 °C |
0.70 µm/km @Temperature 212 °F |
||
| 2.2 µm/km @Temperature 200 °C |
2.2 µm/km @Temperature 392 °F |
||
| 2.9 µm/km @Temperature 240 °C |
2.9 µm/km @Temperature 464 °F |
||
| Charpy Impact Unnotched | 5.90 J/cm² | 28.1 ft-lb/in² | EN ISO 179/1eU |
| Charpy Impact, Notched | 1.56 J/cm² | 7.42 ft-lb/in² | EN ISO 179/1eA |
| Coefficient of Friction, Dynamic | 0.11 @Temperature 100 °C |
0.11 @Temperature 212 °F |
Dry Operation |
| 0.16 @Temperature 20.0 °C |
0.16 @Temperature 68.0 °F |
Dry Operation | |
| Coefficient of Friction, Static | 0.19 @Temperature 20.0 °C |
0.19 @Temperature 68.0 °F |
Dry Operation |
| Tensile Creep Modulus, 1000 hours | 4320 MPa | 627000 psi | At 1% Deformation; DIN 53444 |
| Limiting Pressure Velocity | 0.54883 MPa-m/sec | 15669 psi-ft/min | v = 1m/min |
| 0.88333 MPa-m/sec | 25219 psi-ft/min | v = 100m/min | |
| 0.933 MPa-m/sec | 26600 psi-ft/min | v = 200m/min | |
| 1.415 MPa-m/sec | 40400 psi-ft/min | v = 10m/min | |
| Compression Set | 4.4 % | 4.4 % | Elastic Compression Limit |
| 10.9 % | 10.9 % | Nominal Compressive Strain at Compressive Strength; DIN EN ISO 604 | |
| 10.9 % | 10.9 % | Nominal Compressive Strain at Break; DIN EN ISO 604 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 27.0 µm/m-°C @Temperature <=100 °C |
15.0 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
| 29.0 µm/m-°C @Temperature <=150 °C |
16.1 µin/in-°F @Temperature <=302 °F |
ISO E 831 | |
| Specific Heat Capacity | 1.06 J/g-°C | 0.253 BTU/lb-°F | DSC |
| Melting Point | 390 °C | 734 °F | DSC |
| Maximum Service Temperature, Air | 250 °C | 482 °F | Pressed Bushings |
| 280 °C | 536 °F | Continuous | |
| 320 °C | 608 °F | Short Term (3h) | |
| Deflection Temperature at 1.8 MPa (264 psi) | 290 °C | 554 °F | DIN EN ISO 75 |
| Glass Transition Temp, Tg | 240 °C | 464 °F | DSC |
| Flammability, UL94 | V-0 | V-0 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 5.00e+6 ohm-cm | 5.00e+6 ohm-cm | IEC 93 |
| Surface Resistance | 3.00e+6 ohm | 3.00e+6 ohm | IEC 93 |
| Dielectric Constant | 3.4 @Frequency 110 Hz |
3.4 @Frequency 110 Hz |
IEC 250 |
| Dielectric Strength | 0.100 kV/mm | 2.54 kV/in | IEC 243 |
| Dissipation Factor | 0.00090 | 0.00090 | IEC 112 |
| 0.080 @Frequency 1.00 Hz |
0.080 @Frequency 1.00 Hz |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Alignment Adjustment | 3 | Nominal Scale: 1, low; 10, high |
| Chemical Sterilization | 10 | Nominal Scale: 1, low; 10, high |
| Color | Green | |
| Creep Resistance | 6 | Nominal Scale: 1, low; 10, high |
| Dimensional Stability with Thermal Expansion | 10 | Nominal Scale: 1, low; 10, high |
| Free from Silicon | Applicable | |
| Gamma-rays Radiation Sterilization | 7 | Nominal Scale: 1, low; 10, high |
| Injection Molded Parts | Applicable | |
| Machined Parts | Applicable | |
| Moist Heat Sterilization | 6 | Nominal Scale: 1, low; 10, high |
| Plastic Granules | Applicable | |
| Resistance Against dust, Dirt, Abrasive Substances | 5 | Nominal Scale: 1, low; 10, high |
| Resistance Against Hot Water | 120 | |
| Resistance to Chemicals | 5 | Nominal Scale: 1, low; 10, high |
| Resistant Against Disinfectant | Applicable | |
| Rods up to Øe (de) | Applicable | |
| ROHS/WEEE | Applicable | |
| Sheets up to Maximum Thickness | Applicable | |
| Sliding Velocity | 350 | |
| Suitable for Outdoor Use | 9 | Nominal Scale: 1, low; 10, high |
| Suitable for Vacuum | Applicable | |
| Tubes (hollow rods) up to Øe (de) | Applicable | |
| UV Rays Resistance | 9 | Nominal Scale: 1, low; 10, high |