Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 19.0 µm/m-°C @Temperature -55.0 - 280 °C |
10.6 µin/in-°F @Temperature -67.0 - 536 °F |
X Direction; IPC-TM-650 2.4.41 |
Rogers Corporation RO4450B Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 500 °C |
10.6 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature -55.0 - 280 °C |
10.6 µin/in-°F @Temperature -67.0 - 536 °F |
X Direction; IPC-TM-650 2.4.41 |
Rogers Corporation RO4450F Prepreg Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
10.6 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® R-7-120NA Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-7-120NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance moldi.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
10.6 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ASTM E831 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature -40.0 - 100 °C |
10.6 µin/in-°F @Temperature -40.0 - 212 °F |
Alpha 1; TMA |
Tra-Con Tra-Bond 526W01 Microelectronics Grade Encapsulant TRA-BOND 526W01 is a one component micro-electronics grade controlled flow encapsulant designed to protect wire bonds and bare die. TRA-BOND 526W01 has a low coefficient of thermal expansion and low.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 20.0 - 50.0 °C |
10.6 µin/in-°F @Temperature 68.0 - 122 °F |
MD |
DuPont Teijin Films Melinex® 377 Polyester Film, 142 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 20.0 - 50.0 °C |
10.6 µin/in-°F @Temperature 68.0 - 122 °F |
MD |
DuPont Teijin Films Melinex® 377 Polyester Film, 200 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 20.0 - 50.0 °C |
10.6 µin/in-°F @Temperature 68.0 - 122 °F |
MD |
DuPont Teijin Films Melinex® 377 Polyester Film, 300 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 20.0 - 50.0 °C |
10.6 µin/in-°F @Temperature 68.0 - 122 °F |
MD |
DuPont Teijin Films Melinex® 377 Polyester Film, 48 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 20.0 - 50.0 °C |
10.6 µin/in-°F @Temperature 68.0 - 122 °F |
MD |
DuPont Teijin Films Melinex® 377 Polyester Film, 500 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 20.0 - 50.0 °C |
10.6 µin/in-°F @Temperature 68.0 - 122 °F |
MD |
DuPont Teijin Films Melinex® 377 Polyester Film, 75 Gauge Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in sta.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature -30.0 - 23.0 °C |
10.6 µin/in-°F @Temperature -22.0 - 73.4 °F |
longitudinal; ASTM E831 |
Bond Laminates TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact .. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature -30.0 - 23.0 °C |
10.6 µin/in-°F @Temperature -22.0 - 73.4 °F |
transverse; ASTM E831 |
Bond Laminates TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact .. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 0.000 - 100 °C |
10.6 µin/in-°F @Temperature 32.0 - 212 °F |
y direction; IPC TM-650 2.4.24 |
Arlon CuClad 250 PTFE/Woven Fiberglass Laminate Microwave Printed Circuit Board Substrate CuClad 250 uses a higher fiberglass/PTFE ratio to provide mechanical properties approaching those of conventional substrates. Better dimensional stability and lower thermal expansion in all directi.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 20.0 - 1000 °C |
10.6 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
CTE, linear | 19.0 µm/m-°C @Temperature 20.0 - 500 °C |
10.6 µin/in-°F @Temperature 68.0 - 932 °F |
|
Industeel URANUS® S1 4 % Si, Austenitic Stainless Steel Resistant to Nitric Acid Solutions Description: Research carried out in about the last fifteen years in CREUSOT LOIRE INDUSTRIE laboratories shows that a strong addition of silicon to austenitic stainless steels of the 18/10 type has.. |