Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 377 Polyester Film, 300 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 377 Polyester Film, 300 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Melinex® 377 is a translucent matte film having a medium surface gloss which is suitable for creating woodgrain and muted metallic effects.Typical Applications: Melinex® is suitable for use in stamping foil, metallizing, and casting/release applications.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 100 MPa

@Strain >=5.00 %
14500 psi

@Strain >=5.00 %
ASTM D882A
Film Tensile Strength at Yield, TD 103 MPa

@Strain >=5.00 %
15000 psi

@Strain >=5.00 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
50% RH; Strain rate 50%/min; ASTM D882-83
Coefficient of Friction, Dynamic 0.30
0.30
A-B; ASTM D1894
Film Tensile Strength at Break, MD 172 MPa
24900 psi
50% RH; Strain rate 50%/min; ASTM D882A
Film Tensile Strength at Break, TD 211 MPa
30600 psi
50% RH; Strain rate 50%/min; ASTM D882A
Thermal Properties Metric English Comments
CTE, linear 16.0 µm/m-°C

@Temperature 20.0 - 50.0 °C
8.89 µin/in-°F

@Temperature 68.0 - 122 °F
TD
19.0 µm/m-°C

@Temperature 20.0 - 50.0 °C
10.6 µin/in-°F

@Temperature 68.0 - 122 °F
MD
Shrinkage, MD 3.0 %

@Temperature 190 °C,
Time 300 sec
3.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 3.0 %

@Temperature 190 °C,
Time 300 sec
3.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 97 %
97 %
ASTM D1003
Gloss 92 %
92 %
45°; ASTM D523
92 %
92 %
60°; ASTM D523
Transmission, Visible 67 %
67 %
TLT; ASTM D1003
Users viewing this material also viewed the following: