Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 200 °C |
6.50 µin/in-°F @Temperature 68.0 - 392 °F |
|
Kennametal Stellite Nucalloy® 453 High-Silicon Nickel-Base Hardfacing Alloy Applications include chemical control valves, nuclear globe valves, nuclear gate valves, nuclear sliding parts, and pressure bars for plywood cutters.Nucalloy® alloys are unique, patented, high-s.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Kennametal Stellite Stellite® 98M2 cast Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Kennametal Stellite Stellite® 98M2 with P/M Processing Adhesive wear test data P/M 0.58 Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.0 - 427 °C |
6.50 µin/in-°F @Temperature 69.8 - 801 °F |
|
Latrobe Lescalloy® 17-4 VAC-ARC Precipitation Hardening Stainless Steel LESCALLOY 17-4 VAC-ARC steel is a precipitation hardening martensitic stainless steel. A wide range of mechanical properties is available via simple aging within a 900-1150°F (482-621°C) tempe.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe LSSâ„¢ 420 MQ Plastic Mold Steel (AISI 420) TLS 420 MQ is a highly-refined, Mold Quality stainless steel that is engineered to exhibit excellent polishability, good corrosion resistance, and good wear resistance. TLS 420 MQ is melted using an.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
Latrobe LSSâ„¢ 420 Supreme Plastic Mold Steel (AISI 420) TLS 420 Supreme is a specially-refined, mold-quality stainless steel that is engineered to provide supreme polishability, good corrosion resistance, and good wear resistance. TLS 420 supreme is manu.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 300 °C |
6.50 µin/in-°F @Temperature 68.0 - 572 °F |
|
Kennametal Stellite Deloro® 50 Nickel Alloy Nickel base. Provides maximum amount of abrasion and metal-on-metal wear resistance for cast components. Superior wear resistance. Adequate corrosion resistance. Tungsten carbide tools allow for mac.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are c.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
HP Alloys Alloy C-276, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 100 °C |
6.50 µin/in-°F @Temperature 68.0 - 212 °F |
|
HP Alloys Alloy C-276, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 432 °C |
6.50 µin/in-°F @Temperature 68.0 - 810 °F |
|
Schmolz + Bickenbach UgiPermâ„¢ 12FM Stainless Steel Bar Description: UgiPermâ„¢ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was develope.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 0.000 - 649 °C |
6.50 µin/in-°F @Temperature 32.0 - 1200 °F |
|
Crucible Steel 416 Plus Chromium Steel Crucible 416 Plus is a hardenable chromium steel to which elements have been added to improve machinability and non-galling characteristics. Better machinability than that of standard AISI Type 4.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.50 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel Holder Block Steel, AISI 4150 Modified Crucible Holder Block is a prehardened (26/30 HRC) free machining medium alloy steel intended for holders or backers for plastic molds, die casting dies, and cold or hot forming tools. It may also b.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.50 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel MAXEL® 3-1/2 (Brake Die) Free-Machining Alloy Steel, AISI 4150 S MAXEL 3-1/2 free-machining alloy steel provides a good combination of heat treated properties and machinability. This alloy steel is manufactured under close quality control to an ASTM grain size of.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 21.1 - 260 °C |
6.50 µin/in-°F @Temperature 70.0 - 500 °F |
|
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 500 °C |
6.50 µin/in-°F @Temperature 68.0 - 932 °F |
|
Bohler-Uddeholm BÖHLER M303 EXTRA Plastic Mold Steel BOHLER M303 EXTRA is a stainless martensitic chromium steel, offering excellent toughness, corrosion and wear resistance. It is characterized by improved machinability and polishability. BOHLER M303.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 200 °C |
6.50 µin/in-°F @Temperature 392 °F |
|
Bohler-Uddeholm BÖHLER S692/S693 MICROCLEAN® PM M4 High Speed Steel Description: S692/S693 MICROCLEAN are high-sulfur and low sulfur versions of high-carbon PM M4 high speed steel that is produced using state-of-the-art “Generation 3” powder processing technology... |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 400 °C |
6.50 µin/in-°F @Temperature 752 °F |
hardened to 58 HRC |
Bohler-Uddeholm UDDEHOLM ELMAX® Powder Metallurgy Stainless Mold Steel High chromium-vanadium-molybdenum alloyed steelA through-hardening corrosion resistant mold steel made by powder metallurgy processing techniques. The high wear resistance makes ELMAX® suitable for.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 399 °C |
6.50 µin/in-°F @Temperature 750 °F |
hardened to 60 HRC |
Bohler-Uddeholm UDDEHOLM VANADIS 4 EXTRA® Powder Metallurgically Produced Tool Steel Description: Uddeholm Vanadis 4 Extra is a chromiummolybdenum-vanadium alloyed steel Vanadis 4 Extra is characterized by: Very good ductility High abrasive-adhesive wear resistance High compressive.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature <=427 °C |
6.50 µin/in-°F @Temperature <=801 °F |
|
AK Steel 15-5 PH® Precipitation Hardening Stainless Steel, Condition H 900 AK Steel 15-5 PH® provides high strength, good corrosion resistance, good mechanical properties at temperatures up to 600°F (316°C), and good toughness in both base metal and welds. Short-time, .. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature -17.8 - 300 °C |
6.50 µin/in-°F @Temperature 0.000 - 572 °F |
|
American Utility Metals Cromgard® Stainless Steel Cromgard is a low cost stainless steel, which is able to provide benefits of good weldability and formability, making it capable of fabrication by conventional techniques. It provides the benefits o.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 400 °C |
6.50 µin/in-°F @Temperature 68.0 - 752 °F |
|
Assab Steels VANADIS 10 Cold Work Steel VANADIS 4 is a chromium-molybdenum-vanadium alloyed steel which is characterized by:Extremely high abrasive wear resistanceHigh compressive strengthVery good through-hardening propertiesGood toughne.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 650 °C |
6.50 µin/in-°F @Temperature 68.0 - 1200 °F |
|
ATI Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed AL 433™ is a stainless steel in the ferritic family of alloys with Type 409 and Type 439. The AL 433 alloy contains 20% chromium for pitting and crevice corrosion resistance in the presence of chl.. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 538 °C |
6.50 µin/in-°F @Temperature 68.0 - 1000 °F |
|
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 11.7 µm/m-°C @Temperature 20.0 - 200 °C |
6.50 µin/in-°F @Temperature 68.0 - 392 °F |
|
Schmolz + Bickenbach Cryodur® 2990 Cold Work Die Steel Description: Newly developed ledeburitic cold-work steel with high hardness, good toughness and high tempering resistance combined with high wear resistance.Applications: Cutting and punching tools .. |