Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.0 µm/m-°C @Temperature -55.0 - 288 °C |
6.11 µin/in-°F @Temperature -67.0 - 550 °F |
Y-Direction; ASTM D3386-94 |
Rogers Corporation RO4533 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature -55.0 - 288 °C |
6.11 µin/in-°F @Temperature -67.0 - 550 °F |
X-Direction; ASTM D3386-94 |
Rogers Corporation RO4534 Ceramic-Filled, Glass-Reinforced Hydrocarbon Laminate The RO4500™ Series Cost Performance Antenna Grade Laminates are ceramic-filled, glass-reinforced hydrocarbon based materials that provides the controlled dielectric constant, low loss performance a.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 500 °C |
6.11 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4016 Ferritic Stainless Steel Fairly good corrosion resistant formable steel in mildly corrosive environments. Oxidation resistant at elevated temperatures (up to ~800°C). Ductile, does not work harden readily, and is well su.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.11 µin/in-°F @Temperature 68.0 - 212 °F |
|
Kennametal Stellite Nucalloy® 453 High-Silicon Nickel-Base Hardfacing Alloy Applications include chemical control valves, nuclear globe valves, nuclear gate valves, nuclear sliding parts, and pressure bars for plywood cutters.Nucalloy® alloys are unique, patented, high-s.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 °C |
6.11 µin/in-°F @Temperature 68.0 °F |
Across Surface; ASTM D-696 |
Glastic GLASTHERM S Insulation Sheet Glastherm Grade S is a general purpose insulation sheet with an economical combination of thermal and physical properties. Not recommended for processes where the continuous operating temperature e.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature >=100 °C |
6.11 µin/in-°F @Temperature >=212 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 0.000 - 100 °C |
6.11 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel SOLEIL C5 13% Cr 4 Ni Martensitic Stainless Steel with Improved Toughness Description: Soleil C5 is a 13% Cr 4 Ni 0.5 Mo martensitic stainless steel. Its nickel content, associated with low carbon ensures better weldability, ductility, impact resistance and fatigue resist.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.11 µin/in-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are c.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 0.000 - 100 °C |
6.11 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel VIRGO 15.5PH 15Cr-5Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour - air cooling) Description: Alloy VIRGO 15.5 PH is a precipitation hardening martensitic stainless steel with 15% Cr, 5% Ni, 3.5% Cu and 0.3% Nb/Cb. The grade combines high mechanical properties and medium corrosi.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.1 - 149 °C |
6.13 µin/in-°F @Temperature 70.0 - 300 °F |
|
Latrobe BG42® Stainless Knife Steel (AMS 5749) LESCALLOY® BG42® VIM VAR is a double vacuum melted martensitic stainless high speed steel designed for critical aerospace structural components and high performance bearings. The steel is vacu.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 1000 °C |
6.11 µin/in-°F @Temperature 68.0 - 1830 °F |
DIN EN 821-1 |
CeramTec ZN 40 Zirconia, ZrO2-MgO ZN 40 is a zirconium oxide ceramic with an excellent surface finish and a higher strength than aluminum oxide. Its good crack resistance and anti-friction properties, combined with steel-like therma.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.10 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel CHRO-MOW® Tool Steel, AISI H12 Chro-Mow is a general purpose hot work tool steel, combining good high-temperature strength with moderate toughness and heat check resistance. It is suited for applications where drastic coolants ar.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 21.1 - 93.3 °C |
6.10 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel CPM® Nu-Die® EZ Tool Steel CRUCIBLE CPM Nu-Die EZ is a new, patented die and mold steel designed for service as die casting dies and plastic injection molds. It is supplied in the prehardened condition, and is easily machined.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.11 µin/in-°F @Temperature 68.0 - 392 °F |
|
Crucible Steel CPM® S35VN™ Stainless Steel CPM S35VN is a martensitic stainless steel designed to offer improved toughness over CPM S30V. It is also easier to machine and polish than CPM S30V. Its chemistry has been rebalanced so that it for.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 95.0 °C |
6.11 µin/in-°F @Temperature 68.0 - 203 °F |
|
Crucible Steel Nu-Die® XL (Premium Quality AISI H13) Tool Steel Nu-Die XL (AISI H13) is a premium version of H13 tool steel manufactured, tested and certified to meet stringent die casting industry specifications issued by NADCA, Chrysler and others. It offers b.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 199 °C |
6.10 µin/in-°F @Temperature 390 °F |
hardened to 52 HRC |
Bohler-Uddeholm POLMAX® 420 Modified - Stainless Mold Steel Polmax is an excellent choice for extreme surface finish requirements. This high performance grade achieves surface finishes that go well beyond conventional tool steels. Polmax is specifically eng.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 199 °C |
6.10 µin/in-°F @Temperature 390 °F |
hardened to 50 HRC |
Bohler-Uddeholm UDDEHOLM STAVAX® ESR Modified 420 Premium grade stainless tool steelStavax® ESR is characterized by: Good corrosion resistance Good polishability Good wear resistance Good machinability Good stability in hardeningApplications: Udd.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 600.0 °C |
6.10 µin/in-°F @Temperature 1112 °F |
hardened and tempered |
Bohler-Uddeholm UDDEHOLM VANADIS 60 Powder Metallurgically Produced Tool Steel Uddeholm Vanadis 60 is a high alloyed powder metallurgical high speed steel suitable for very demanding cold work applications and for cutting tools. The high carbon and alloying content, Co, Mo, W .. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature <=538 °C |
6.11 µin/in-°F @Temperature <=1000 °F |
|
AK Steel PH 15-7 Mo® Precipitation Hardening Stainless Steel, Condition RH 950 AK Steel 15-7 Mo® provides high strength and hardness, good corrosion resistance and minimum distortion on heat treatment. It is easily formed in the annealed condition and develops effective bala.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 27.0 - 93.0 °C |
6.11 µin/in-°F @Temperature 80.6 - 199 °F |
|
Carpenter No. 883® Hot Work Die Steel (Red-Tough) (AISI H13) No. 883 hot work die steel is a 5% chromium hot work tool steel designed particularly for applications requiring extreme toughness combined with good red-hardness. It has given an extra margin of sa.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 25.0 - 538 °C |
6.11 µin/in-°F @Temperature 77.0 - 1000 °F |
|
Carpenter Thermo-Span® Fe-Co-Ni Superalloy Data provided by Carpenter Technology Corporation.Thermo-Span® alloy is a precipitation hardenable superalloy which exhibits a low coefficient of thermal expansion over a broad temperature range, h.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 27.0 °C |
6.11 µin/in-°F @Temperature 80.6 °F |
|
ATI Allegheny Ludlum AL 601™ Nickel-Base Alloy, Annealed at 982°C (1800°F), UNS N06601 Allegheny Ludlum's AL 601 alloy is an austenitic nickel-chromium-iron alloy designed for both heat and corrosion resistance. As compared to AL 600 alloy, the AL 601 alloy has, in addition to increa.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 250 °C |
6.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Fecralloy™ 135 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire, bar, and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small .. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 250 °C |
6.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Fecralloy™ Electrical Resistance Steel Yttrium addition does not appear in nominal composition. Ferritic stainless steel with aluminum. Available as wire, bar, tube, and strip. Used mainly for electrical elements in both industrial and.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 250 °C |
6.11 µin/in-°F @Temperature 68.0 - 482 °F |
|
Resistalloy International Fecralloy™ 134 Electrical Resistance Steel Ferritic stainless steel with aluminum. Available as wire and strip. Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small labora.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 0.000 - 100 °C |
6.11 µin/in-°F @Temperature 32.0 - 212 °F |
|
Industeel VIRGO 17.4PH 17Cr-4Ni-3Cu Precipitation Hardening Martensitic Stainless Steel (480°C (900°F) - 1 hour + air cooled) Description: Alloy VIRGO 17.4 PH is a precipitation hardening martensitic stainless steel with Cu and Nb/Cb additions. The grade combines high strength, hardness (up to 300°C / 572°F) and corrosio.. |