| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Brinell | <= 229 | <= 229 | |
| Hardness, Rockwell C | <= 53 | <= 53 | |
| Hardness, Vickers | 300 @Temperature 316 °C |
300 @Temperature 600 °F |
|
| 400 @Temperature 204 °C |
400 @Temperature 400 °F |
||
| 410 @Temperature 93.3 °C |
410 @Temperature 200 °F |
||
| 500 @Temperature -3.89 °C |
500 @Temperature 25.0 °F |
||
| Tensile Strength, Ultimate | 950 MPa @Temperature 600 °C |
138000 psi @Temperature 1110 °F |
|
| 1350 MPa @Temperature 400 °C |
196000 psi @Temperature 752 °F |
||
| 1590 MPa @Temperature 200 °C |
231000 psi @Temperature 392 °F |
||
| 1610 MPa @Temperature 25.0 °C |
234000 psi @Temperature 77.0 °F |
||
| Tensile Strength, Yield | 410 MPa @Temperature 316 °C |
59500 psi @Temperature 600 °F |
|
| 1200 MPa @Temperature 204 °C |
174000 psi @Temperature 400 °F |
||
| 1350 MPa @Temperature 93.3 °C |
196000 psi @Temperature 200 °F |
||
| 1500 MPa @Temperature -3.89 °C |
218000 psi @Temperature 25.0 °F |
||
| Elongation at Yield | 12 % @Temperature -3.89 °C |
12 % @Temperature 25.0 °F |
|
| 13 % @Temperature 93.3 °C |
13 % @Temperature 200 °F |
||
| 15 % @Temperature 204 °C |
15 % @Temperature 400 °F |
||
| 21 % @Temperature 316 °C |
21 % @Temperature 600 °F |
||
| Reduction of Area | 52 % @Temperature -3.89 °C |
52 % @Temperature 25.0 °F |
|
| 53 % @Temperature 93.3 °C |
53 % @Temperature 200 °F |
||
| 55 % @Temperature 204 °C |
55 % @Temperature 400 °F |
||
| 65 % @Temperature 316 °C |
65 % @Temperature 600 °F |
||
| Charpy Impact Unnotched | 50.0 J/cm² @Temperature -3.89 °C |
238 ft-lb/in² @Temperature 25.0 °F |
|
| 70.0 J/cm² @Temperature 93.3 °C |
333 ft-lb/in² @Temperature 200 °F |
||
| 80.0 J/cm² @Temperature 204 °C |
381 ft-lb/in² @Temperature 400 °F |
||
| 85.0 J/cm² @Temperature 316 °C |
405 ft-lb/in² @Temperature 600 °F |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 11.0 µm/m-°C @Temperature >=100 °C |
6.11 µin/in-°F @Temperature >=212 °F |
|
| 11.8 µm/m-°C @Temperature >=300 °C |
6.56 µin/in-°F @Temperature >=572 °F |
||
| 12.4 µm/m-°C @Temperature >=500 °C |
6.89 µin/in-°F @Temperature >=932 °F |
||
| 13.1 µm/m-°C @Temperature >=700 °C |
7.28 µin/in-°F @Temperature >=1290 °F |
||
| Thermal Conductivity | 27.6 W/m-K @Temperature 25.0 °C |
192 BTU-in/hr-ft²-°F @Temperature 77.0 °F |
|
| 29.3 W/m-K @Temperature 400 °C |
203 BTU-in/hr-ft²-°F @Temperature 752 °F |
||
| 29.3 W/m-K @Temperature 600 °C |
203 BTU-in/hr-ft²-°F @Temperature 1110 °F |
||
| 31.0 W/m-K @Temperature 200 °C |
215 BTU-in/hr-ft²-°F @Temperature 392 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Carbon, C | 0.39 % | 0.39 % | |
| Chromium, Cr | 5.0 % | 5.0 % | |
| Iron, Fe | >= 88.61 % | >= 88.61 % | |
| Manganese, Mn | <= 1.5 % | <= 1.5 % | |
| Molybdenum, Mo | 2.0 % | 2.0 % | |
| Silicon, Si | <= 1.5 % | <= 1.5 % | |
| Vanadium, V | 1.0 % | 1.0 % |