Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 10.3 µm/m-°C @Temperature 25.0 - 100 °C |
5.72 µin/in-°F @Temperature 77.0 - 212 °F |
|
Osprey Metals CE11 Al-Si Controlled Expansion Alloy Al-50%Si controlled expansion alloy manufactured and patented by Osprey Metals Ltd.Information provided to MatWeb by Osprey Metals. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 900 °C |
5.72 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton 838 Zirconia + 3 mol% Yttria (YSZ) Brand 838 features: Co-precipitation; high strength.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, .. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 900 °C |
5.72 µin/in-°F @Temperature 1650 °F |
|
MarkeTech Repton 848 Zirconia + 3 mol% Yttria (YSZ) REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 38.0 - 260 °C |
5.72 µin/in-°F @Temperature 100 - 500 °F |
|
Latrobe LSSâ„¢ D2 Tool Steel (ASTM D2) TLS D2 tool steel is a versatile high-carbon, high-chromium, air-hardening tool steel that is characterized by a relatively high attainable hardness and numerous, large, chromium rich alloy carbides.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 100 °C |
5.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
Latrobe 14-4CrMo Stainless Tool Steel 14-4CrMo is a wear resistant, martensitic stainless tool steel that exhibits better corrosion resistance than Type 440C stainless steel. The molybdenum in the steel provides superior corrosion resis.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 93.0 °C |
5.72 µin/in-°F @Temperature 68.0 - 199 °F |
|
HP Alloys Alloy B-2, Solution Treated, 10% Cold Worked Solution Treated, 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 93.0 °C |
5.72 µin/in-°F @Temperature 68.0 - 199 °F |
|
HP Alloys Alloy B-2, Solution Treated, 20% Cold Worked Solution Treated, 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 93.0 °C |
5.72 µin/in-°F @Temperature 68.0 - 199 °F |
|
HP Alloys Alloy B-2, Solution Treated, 30% Cold Worked Solution Treated, 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 93.0 °C |
5.72 µin/in-°F @Temperature 68.0 - 199 °F |
|
HP Alloys Alloy B-2, Solution Treated, 40% Cold Worked Solution Treated, 40% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 300 °C |
5.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF6 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 300 °C |
5.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-SF6HT Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 100 °C |
5.75 µin/in-°F @Temperature 68.0 - 212 °F |
|
Schmolz + Bickenbach UgiPermâ„¢ 12FM Stainless Steel Bar Description: UgiPermâ„¢ 12FM is a 12% chrome ferritic stainless with improved magnetic properties designed for use in electro-injectors, valves and many other applications. The grade was develope.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 0.000 - 100 °C |
5.70 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 420 and 420F Chromium Steel Crucible 416 Plus is a hardenable chromium steel which is the general purpose cutlery grade. This grade is magnetic in all conditions. Information provided by Crucible Specialty Metals. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 100 °C |
5.70 µin/in-°F @Temperature 68.0 - 212 °F |
|
Crucible Steel 430F Stainless Steel Crucible 430F is a low carbon, high chromium ferritic stainless steel, specially developed for solenoid core applications in corrosive environments. The chemistry is closely controlled to develop o.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature -17.8 - 93.3 °C |
5.70 µin/in-°F @Temperature 0.000 - 200 °F |
|
Crucible Steel 440A Chromium Steel Crucible 440A is a hardenable chromium steel which is the toughest of the high chromium cutlery grades. This grade is magnetic at all times. Information provided by Crucible Specialty Metals. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 26.7 - 93.3 °C |
5.70 µin/in-°F @Temperature 80.0 - 200 °F |
|
Crucible Steel 440B Chromium Steel Crucible 440B Is a hardenable chromium steel which is cutlery grade having high attainable hardness and toughness. This grade is magnetic at all times. Information provided by Crucible Specialty Me.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 0.000 - 100 °C |
5.70 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 440C Chromium Steel Crucible 440C is a hardenable chromium steel. It has one of the highest attainable hardnesses of the corrosion and heat resisting grades. This grade is magnetic at all times.Information provided b.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 0.000 - 100 °C |
5.72 µin/in-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel CSM® 420 XL Stainless Steel CSM 420 XL is the workhorse premium quality stainless mold steel designed for applications requiring a combination of corrosion resistance and wear resistance. It is double melted for the microstruc.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 21.1 - 93.3 °C |
5.70 µin/in-°F @Temperature 70.0 - 200 °F |
|
Crucible Steel PEERLESS A Tool Steel, AISI H21 Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 300 °C |
5.72 µin/in-°F @Temperature 572 °F |
|
Bohler-Uddeholm BÖHLER S290 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 21.0 - 93.0 °C |
5.72 µin/in-°F @Temperature 69.8 - 199 °F |
|
AK Steel 17-7 PH® Precipitation Hardening Stainless Steel, Condition RH 950 AK Steel 17-7 PH® provides high strength and hardness, excellent fatigue properties, good corrosion resistance, good formability, and minimum distortion upon heat treatment. This alloy provides va.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 25.0 - 38.0 °C |
5.72 µin/in-°F @Temperature 77.0 - 100 °F |
|
Carpenter Stentor® Alloy Tool Steel (Oil-Hard) (AISI 02) An oil-hardening alloy with excellent size change properties, Stentor tool steel is especially suited for general purpose work in the toolroom. It is safe to harden, and shows little size change or .. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 100 °C |
5.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
ATI Allegheny Ludlum 430 Ferritic Stainless Steel Characteristics:oxidation resistant at elevated temperatures, corrosion resistance approaching nickel-bearing stainless steels in mildly corrosive environments, ductile, does not work harden readily.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 300 °C |
5.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
ATI Allegheny Ludlum Type 441 Alloy Stainless Steel Allegheny Ludlum stainless Type 441 alloy is a heat resisting ferritic grades providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dual stab.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 300 °C |
5.72 µin/in-°F @Temperature 68.0 - 572 °F |
Type 441 |
ATI Allegheny Ludlum Type AL 441HP™ Stainless Steel Alloy Allegheny Ludlum stainless Type AL 441HP™ alloy is a heat resisting ferritic grade providing good oxidation and corrosion resistance for applications like automotive exhaust system components. Dua.. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 93.0 °C |
5.72 µin/in-°F @Temperature 68.0 - 199 °F |
|
HP Alloys Alloy B-2, Solution Treated, 50% Cold Worked Solution Treated, 50% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc. and Haynes International. |
|||
CTE, linear | 10.3 µm/m-°C @Temperature 20.0 - 300 °C |
5.72 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott BG26 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |