Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 40.0 - 80.0 µm/m-°C | 22.2 - 44.4 µin/in-°F | Average value: 58.0 µm/m-°C Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
CTE, linear, Transverse to Flow | 17.0 - 80.0 µm/m-°C | 9.44 - 44.4 µin/in-°F | Average value: 55.4 µm/m-°C Grade Count:12 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
CTE, linear, Transverse to Flow | 26.4 - 80.0 µm/m-°C | 14.7 - 44.4 µin/in-°F | Average value: 58.5 µm/m-°C Grade Count:7 |
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma.. |
|||
CTE, linear, Transverse to Flow | 70.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
BASF Ultramid® B3ZG3 BK30564 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 BK30564 is an impact-modified, pigmented black, 15% glass fiber reinforced injection molding PA6 grade. |
|||
CTE, linear, Transverse to Flow | 70.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry) Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi.. |
|||
CTE, linear, Transverse to Flow | 70.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B35EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
CTE, linear, Transverse to Flow | 70.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
CTE, linear, Transverse to Flow | 70.0 - 80.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
38.9 - 44.4 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
CTE, linear, Transverse to Flow | 45.0 - 80.0 µm/m-°C | 25.0 - 44.4 µin/in-°F | Average value: 65.5 µm/m-°C Grade Count:10 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
CTE, linear, Transverse to Flow | 10.0 - 80.0 µm/m-°C | 5.56 - 44.4 µin/in-°F | Average value: 33.3 µm/m-°C Grade Count:3 |
Overview of materials for Nylon 66, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Nucleated". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
CTE, linear, Transverse to Flow | 40.0 - 80.0 µm/m-°C | 22.2 - 44.4 µin/in-°F | Average value: 59.3 µm/m-°C Grade Count:21 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear, Transverse to Flow | 45.0 - 80.0 µm/m-°C | 25.0 - 44.4 µin/in-°F | Average value: 62.8 µm/m-°C Grade Count:18 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
CTE, linear, Transverse to Flow | 37.0 - 80.0 µm/m-°C | 20.6 - 44.4 µin/in-°F | Average value: 50.4 µm/m-°C Grade Count:5 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |