Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 101 µm/m-°C @Temperature 23.0 - 60.0 °C |
56.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36R PA6.12 (Europe-Africa-Middle East) Internally lubricated PA6.12, containing Glass Fiber and PTFE |
|||
CTE, linear, Transverse to Flow | 101 µm/m-°C @Temperature -30.0 - 100 °C |
56.1 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
CTE, linear, Transverse to Flow | 101 µm/m-°C @Temperature 23.0 - 60.0 °C |
56.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant. |
|||
CTE, linear, Transverse to Flow | 101 µm/m-°C @Temperature 23.0 - 60.0 °C |
56.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.This data was suppl.. |
|||
CTE, linear, Transverse to Flow | 101 µm/m-°C @Temperature -30.0 - 30.0 °C |
56.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP IF004 PA6.12 LNP* THERMOCOMP* IF004 is a compound based on Nylon 6/12 resin containing 20% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 101 µm/m-°C @Temperature -30.0 - 30.0 °C |
56.1 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP MX06402H PP LNP* THERMOCOMP* MX06402H is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, Low Extractable. |
|||
CTE, linear, Transverse to Flow | 101 µm/m-°C @Temperature 23.0 - 60.0 °C |
56.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp RFB24 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RFB24 is a compound based on PA 66 resin containing Glass Bead, Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 101 µm/m-°C @Temperature 23.0 - 60.0 °C |
56.1 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide RFB24 PA66, 20/10% Glass Fiber/Glass Bead Filled Injection Molded RFB24 is a Glass Bead and Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as Staramide 66 2010VK Z3)Information provided by Polymer Technology & Services, the North American.. |