Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -30.0 - 120 °C |
35.6 µin/in-°F @Temperature -22.0 - 248 °F |
ISO 11359 |
Nyco NYGLOS® 4W STO105 Wollastonite in Polypropylene Data for polypropylene reinforced with 15% Nyco NYGLOS® 4W STO105 Wollastonite. Polypropylene used is Braskem TI6200Q High Impact Copolymer 20 MFR -NBWollastonite (calcium metasilicate, or CaSiO3).. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX1619 PC Lexan* LUX1619 Polycarbonate resin is an extrusion grade. It is UL94 HB rated. It was designed for high light reflectance. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX2619 PC Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East) Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Asia Pacific) LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Faradex NS0039 PC/ABS (Europe-Africa-Middle East) LNP* Faradex* NS0039 is a compound based on PC/ABS resin containing Flame Retardant, Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, Flame Reta.. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
35.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF0335 PC (Europe-Africa-Middle East) LNP* Lubricomp* LEXAN_LF0335 compound is a 35% glass fiber, milled glass reinforced PC injection moulding resin with improved wear resistance and reduced friction. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
35.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DF006ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF006ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP DX10311 PC (Asia Pacific) DX10311 is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
35.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS Blend resin containing Glass Fiber |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East) XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
35.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP VERTON RX10409D PA 66 LNP* VERTON* RX10409D is a compound based on Nylon 66 containing proprietary fillers. Added feature of this grade is: Structural. |
|||
CTE, linear, Transverse to Flow | 64.0 µm/m-°C | 35.6 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G15HSL NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G15HSL NC010 is a 15% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
CTE, linear, Transverse to Flow | 64.1 µm/m-°C @Temperature -30.0 - 30.0 °C |
35.6 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6 LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers. |
|||
CTE, linear, Transverse to Flow | 64.0 - 70.0 µm/m-°C | 35.6 - 38.9 µin/in-°F | Average value: 66.0 µm/m-°C Grade Count:3 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |