Polymer Property : Glass Transition Temp, Tg = 464 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 240 °C
464 °F
TMA; IPC-TM-650.2.4.24c
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg
The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a..
Glass Transition Temp, Tg 240 °C
464 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Park Electrochemical Nelco® N4000-13 BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg
The Nelco N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. The Nelco N4000-13 BC® is offered as a..
Glass Transition Temp, Tg 240 °C
464 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg
Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides..
Glass Transition Temp, Tg 240 °C
464 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Park Electrochemical Nelco® N4000-13 High-Speed Multifunctional Epoxy Laminate and Prepreg
The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic..
Glass Transition Temp, Tg 240 °C
464 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Park Electrochemical Nelco® N4000-13 SI® High-Speed Multifunctional Epoxy Laminate and Prepreg
The Nelco® N4000-13 series is an enhanced epoxy resin system engineered to provide both outstanding thermal and high signal speed / low signal loss properties. N4000-13 SI® is excellent for applic..
Glass Transition Temp, Tg 240 °C
464 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy
The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,..
Glass Transition Temp, Tg 240 °C
464 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Park Electrochemical Nelco® N4380-13 RF Microwave Performance, Modified Epoxy
The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,..
Glass Transition Temp, Tg 240 °C
464 °F
TMA; IPC-TM-650.2.4.24c
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg
The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a..
Glass Transition Temp, Tg 240 °C
464 °F
DSC
Wolf Kunststoff ZEDEX® ZX-750V5KF 055 Polymer Alloy. Fiber Reinforced
Main Characteristics: Stiff; High elongation and yield stress; Low thermal expansion; Impact resistantApplications: Textile Machinery; Compressors; Hinges; Handling; Machine Tools; Automitve Technol..
Glass Transition Temp, Tg 240 °C
464 °F
DSC
Wolf Kunststoff ZEDEX® ZX-750V5T A9T Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High dimensional stability; High fatigue strength; High weather resistance; Good fire behavior; Suitable for vacuum; Good machinability; Contains PTFE; Stre..