Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 180 - 190 °C | 356 - 374 °F | TMA; IPC-TM-650 2.4.24 |
Rogers Corporation Theta® MCL-HE-679G Laminate, GHA-679G Prepreg Halogen-Free, Low Dielectric Constant, High heat Resistant Multi-Layer Circuit Material Theta® circuit materials are halogen free and have good dielectric characteristics suitable for high speed digital applications. Theta materials, in part due to their superior heat resistance, hav.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | Laminate; standard cure |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | Laminate; standard cure |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | Laminate; standard cure |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 3k 5HS Carbon Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | Laminate; standard cure |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | Laminate; standard cure |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | Midpoint; ISO 11357 |
Victrex® WG102™ Polyaryletherketone Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | Tg |
Industrial Laminates/Norplex MC511A Glass Fabric Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures ar.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | Tg |
Industrial Laminates/Norplex NP511ES Glass Epoxy Laminate Description: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a con.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | |
Polyplastics TOPAS® 6017 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) Possesses the highest heat resistance among cyclic olefin-type resins.Information provided by PolyPlastics. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | DMA |
Hexcel® HexPly® EH25 180°C Curing Epoxy Matrix HexPly® EH25 is a high performance, tough 180°C curing matrix for us in aerospace primary structures. HexPly® EH25 is a self-extinguishing epoxy resin with controlled flow. HexPly® EH25 prepregs.. |
|||
Glass Transition Temp, Tg | 180 °C | 356 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |