Material Notes:
Description: MC511A is a high strength, glass epoxy laminate that is specially formulated to meet power generation producer's exacting standards where higher strength at elevated temperatures are required.MC511A complies with MIL-I-24768/3 – GEB.Thickness Tested: 0.062", 0.125" & 0.500"
Physical Properties Metric English Comments
Density 1.91 g/cc
0.0690 lb/in³
Moisture Absorption at Equilibrium 0.10 %

@Thickness 3.17 mm
0.10 %

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 105 - 125

@Thickness 1.57 mm
105 - 125

@Thickness 0.0620 in
Flexural Strength 255 MPa
37000 psi
at Elevated Temperature (LW E-1/150, T-150)
421 MPa

@Thickness 3.17 mm
61000 psi

@Thickness 0.125 in
CW
493 MPa

@Thickness 3.17 mm
71500 psi

@Thickness 0.125 in
LW
Izod Impact, Unnotched 5.87 J/cm

@Thickness 12.7 mm
11.0 ft-lb/in

@Thickness 0.500 in
LW, Cond E-48/50
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 180 °C
356 °F
Tg
UL RTI, Electrical 170 °C
338 °F
UL RTI, Mechanical without Impact 180 °C
356 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 5.00e+10 ohm-cm
5.00e+10 ohm-cm
Surface Resistance 1.50e+10 ohm
1.50e+10 ohm
Dielectric Constant 4.5

@Thickness 1.57 mm
4.5

@Thickness 0.0620 in
Permittivity
Dielectric Breakdown 65000 V
65000 V
Dissipation Factor 0.028

@Thickness 1.57 mm
0.028

@Thickness 0.0620 in
Arc Resistance 185 sec
185 sec
ASTM D495
Descriptive Properties Value Comments
Bond Strength 2,200 lb