Thermal Properties Metric English Comments
Glass Transition Temp, Tg 160 °C
320 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Park Electrochemical Nelco® N4000-7 SI® FR-4 Epoxy Laminate and Prepreg
The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil..
Glass Transition Temp, Tg 160 °C
320 °F
DMA, ASTM D4065
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC
QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper..
Glass Transition Temp, Tg 160 °C
320 °F
DSC
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade
Amber pelletsInformation provided by Infinite Polymer System II.
Glass Transition Temp, Tg 160 °C
320 °F
DSC
Performance Polymers IPS II PPL-C4219 PEKK (Polyetherketoneketone) Linear Wear Grade
Black pellets; Carbon fiber/PTFE/Graphite compoundInformation provided by Infinite Polymer System II.
Glass Transition Temp, Tg 160 °C
320 °F
DSC
Performance Polymers IPS II PPL-C4250 PEKK (Polyetherketoneketone) Linear 30% Carbon Fiber Reinforced Molding Grade
Black pelletsInformation provided by Infinite Polymer System II.
Glass Transition Temp, Tg 160 °C
320 °F
DSC
Performance Polymers IPS II PPL-C4270 PEKK (Polyetherketoneketone) Linear 40% Carbon Fiber Reinforced Molding Grade
Black pelletsInformation provided by Infinite Polymer System II.
Glass Transition Temp, Tg 160 °C
320 °F
Average value: 160 °C Grade Count:4
Overview of materials for PEKK, Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M..
Glass Transition Temp, Tg 160 °C
320 °F
DMA (Tan d Peak); IPC-TM-650.2.4.24.3
Park Electrochemical Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg
The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil..
Glass Transition Temp, Tg 160 °C
320 °F
Midpoint; ISO 11357
Victrex® HT™ P22 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact compliantInfo..
Glass Transition Temp, Tg 160 °C
320 °F
Midpoint; ISO 11357
Victrex® HT™ P22PF Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, easy flow, FDA food contact compliantInfo..
Glass Transition Temp, Tg 160 °C
320 °F
Midpoint
Victrex® HT™ P45 Polyetherketone
Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, co..
Glass Transition Temp, Tg 160 °C
320 °F
Midpoint; ISO 11357
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp..
Glass Transition Temp, Tg 160 °C
320 °F
Midpoint; ISO 11357
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia..
Glass Transition Temp, Tg 160 °C
320 °F
DSC
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber
AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621..
Glass Transition Temp, Tg 160 °C
320 °F
Cosmic Plastics E4940 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade
Data provided by the manufacturer.
Glass Transition Temp, Tg 160 °C
320 °F
Polyplastics TOPAS® 6015 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade)
A similar grade to 6013. However, heat deflection temperature is (HDT/B) = 150°C. This is a temperature that cannot be achieved with many other amorphous polymers.Information provided by PolyPlasti..
Glass Transition Temp, Tg 160 °C
320 °F
DSC
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Glass Transition Temp, Tg 160 °C
320 °F
DSC
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade
Amber pellets; neat resinInformation provided by Infinite Polymer System II.
Glass Transition Temp, Tg 160 °C
320 °F
ASTM D3418
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr..
Glass Transition Temp, Tg 160 °C
320 °F