Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 150CA30 30% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, FDA food contact c.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 150P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact complian.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 150UF10 Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for composite manufacture, easy flow, FDA food contact compliant.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 150XF Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, fine powder for compression moulding, easy flow, FDA food contact compliant, .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Glass Transition Temp, Tg | >= 143 °C | >= 289 °F | Onset; ISO 11357 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Glass Transition Temp, Tg | >= 143 °C | >= 289 °F | Onset; ISO 11357 |
Victrex® PEEK 650P PolyEtherEtherKetone High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, color natural.Info.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 90CA30 Polyetheretherketone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food cont.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | ISO 11357 |
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | ISO 11357 |
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Victrex® Vicote® 705 Black Polyetheretherketone (PEEK) Powder Coating VICOTE 705Blk is a black pigmented version of the 705 grade. This grade has a nominal particle size of about 50 microns. The powder is dark grey in colour and is a low melt viscosity grade for low.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | |
Zeus PEEK Tubing PEEK (polyetheretherketone) is a high-performance engineered polymer with excellent endurance to heat and one of the highest strength-to-weight ratios of any thermoplastic. This material can be used.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | After 1 hr at 120°C DSC 20°C/min |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix HexPly® M47 is a toughened, self extinguishing 140ºC curing epoxy resin matrix that has been developed for the performance car market. It exhibits good strength retention at elevated temperature, .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® FU1007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | dynamic; DIN 53 736 |
Hippe PEEK Polyetheretherketone PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | ISO 11357-1 |
Murtfeldt Murpec® SP Polyetheretherketone Modified Murpec® SP provides excellent slide properties in addition to good mechanical properties. Murpec® SP also offers improved wear behavior due to its special additives.Special Properties:• .. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | Onset; ISO 11357 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Glass Transition Temp, Tg | >= 143 °C | >= 289 °F | Onset; ISO 11357 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Victrex® Vicote® 701 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Victrex® Vicote® 703 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |
|||
Glass Transition Temp, Tg | 143 °C | 289 °F | DSC |
Victrex® Vicote® 705 Polyetheretherketone (PEEK) Powder Properties: VICOTE 701-707 grades are specially developed powder coatings. They are available in various average particle sizes from 10 - 50 microns. The powders are off-white in color and are avail.. |