Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 108 °C | 226 °F | DAM (SSYS) |
Proto3000 ABS-M30 Fused Deposition Modeling Polymer Description: ABS-M30 is up to 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual modeling, functional prototyping, manufacturing tools, and end-use-parts. ABS.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | DAM (SSYS) |
Proto3000 ABS-M30i Fused Deposition Modeling Polymer Description: ABS-M30i is a high strength material well suited for the medical, pharmaceutical and food packaging industries. Parts manufactured with ABS-M30i material are biocompatible (ISO 10993 ce.. |
|||
Glass Transition Temp, Tg | 108 - 127 °C | 226 - 261 °F | Average value: 116 °C Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Glass Transition Temp, Tg | 108 - 109 °C | 226 - 228 °F | Average value: 108 °C Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | 10°C/min test |
Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stabili.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | 10°C/min test |
Polimeri Europa SINKRAL B733/E ABS, Impact & Heat Stabilized Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,095-04-35-15 Very high impact resistant grade for sheet extrusion with good processability and high thermal sta.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | 10°C/min test |
Polimeri Europa SINKRAL PD G523 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-25-20 High impact injection moulding grade. Other characteristics: good flow, excellent thermal stabilit.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | |
Eastman Tenite 132E-28 Cellulose Acetate
(discontinued **) 28% Plasticized with 25% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical. |
|||
Glass Transition Temp, Tg | 108 - 150 °C | 226 - 302 °F | Average value: 136 °C Grade Count:5 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | ASTM D3418 |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | |
SABIC Innovative Plastics XYLEX EXXX0292 PC+POLYESTER (Europe-Africa-Middle East) XYLEX* EXXX0292 is a transparent copolyester/polycarbonate blend with high flow, V2 UL94 rating at 1.5mm and Tg of 108 C |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | DSC (SSYS) |
Stratasys® ABS-M30 ABS-M30 is 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual prototyping, design verification, and direct digital manufacturing. ABS-M30 has greater tensile,.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | DSC |
Stratasys® ABS-M30i ABS-M30i is a high strength material well suited for the medical, pharmaceutical
and food packaging industries. Parts manufactured with ABS-M30i material
are biocompatible (ISO 10993 certified) an.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | 10°C/min test |
Polimeri Europa SINKRAL F233 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-15-16-25 Medium heat injection moulding grade having high flow and good thermal stability during processing.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | 10°C/min test |
Polimeri Europa SINKRAL PD G120 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-09-30 General purpose injection moulding grade. Characteristics: outstanding rigidity very high surface.. |
|||
Glass Transition Temp, Tg | 108 °C | 226 °F | 10°C/min test |
Polimeri Europa SINKRAL G323 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-20 General purpose injection moulding grade. Main properties are: good impact resistance high flow e.. |