Thermal Properties Metric English Comments
Glass Transition Temp, Tg 105 °C
221 °F
TM R050-25
Resinlab® EP1320 Heat Cure Epoxy Conformal Coating
Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the..
Glass Transition Temp, Tg 105 °C
221 °F
10°C/min test
Polimeri Europa SINKRAL G320 ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SI..
Glass Transition Temp, Tg 105 °C
221 °F
10°C/min test
Polimeri Europa SINKRAL PD M323 ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose injection moulding grade that exhibits outstanding flow and thermal stability duri..
Glass Transition Temp, Tg 105 °C
221 °F
Eastman Tenite 383A-10 Cellulose Acetate Propionate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Glass Transition Temp, Tg 105 °C
221 °F
Mallard Creek Polymers Rovene® 6115 Resin Supported Emulsion
Rovene® 6115 is a hard, non-film forming vehicle that is neutralized with sodium hydroxide for flexographic and gravure inks and overprint varnishes primarily for use on paper and paperboard subs..
Glass Transition Temp, Tg 105 °C
221 °F
ASTM D3418
Kolon DIAMAT® EH
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Glass Transition Temp, Tg 105 °C
221 °F
ASTM D3418
Kolon DIAMAT® IG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Glass Transition Temp, Tg 105 °C
221 °F
Perkin-Elmer DSC-2
Lord Adhesives Thermosetâ„¢ MD-200 Electrically Conductive Die-Attach Adhesive
This is a system with the versatility to fit a wide variety of production and performance needs. The working life allows sufficient time for short production interruption. It can be initially cured ..
Glass Transition Temp, Tg 105 °C
221 °F
MCI Method
Mitsui APELâ„¢ APL6011T Cyclo Olefin Copolymer (COC)
This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces..
Glass Transition Temp, Tg 105 °C
221 °F
Lucite International Colacryl ® LS200 Specialty Acrylic Resin
Colacryl® LS200 is a medium-high molecular weight methyl methacrylate polymer. It is used mainly in coating applications where abrasion resistance and resistance to plasticiser migration are impo..
Glass Transition Temp, Tg 105 °C
221 °F
Lucite International Colacryl ® TS2082 Acrylic Resin
Colacryl® TS2082 is a solid bead resin with low residual peroxide content, specially designed for use in a variety of industrial and dental applications. In dental applications the product is typ..
Glass Transition Temp, Tg 105 °C
221 °F
Lucite International Elvacite ® 2008 Acrylic Resin
Elvacite® 2008 is a low molecular weight methyl methacrylate copolymer. It is used in lacquers and gravure inks requiring low viscosity at high solids. 2008 provides good activity for pigment dis..
Glass Transition Temp, Tg 105 °C
221 °F
Lucite International Elvacite ® 2051 Acrylic Resin
Elvacite® 2051 is a high molecular weight methyl methacrylate polymer. It is used in many coatings applications providing maximum abrasion resistance, block resistance, and slip. It is non-reacti..
Glass Transition Temp, Tg 105 °C
221 °F
Lucite International Elvacite ® 3000 Acrylic Resin
Elvacite® 3000 is a solid bead resin specially designed for use in coatings and inks on a variety of substrates. It has fair compatibility with many binders and plasticisers, and has excellent so..
Glass Transition Temp, Tg 105 °C
221 °F
wet
Henkel Hysol PL 696 Film Adhesive
Epoxy-based structural film adhesive designed primarily for out-of-autoclave curing process applications requiring low cure temperatures as well as low curing pressures and is also available in ligh..
Glass Transition Temp, Tg 105 °C
221 °F
Lucite International Elvacite ® 2041 Acrylic Resin
Elvacite® 2041 is a high molecular weight methyl methacrylate polymer. It is used in many coatings applications providing maximum abrasion resistance, block resistance, and slip. It is non-reacti..
Glass Transition Temp, Tg 105 °C
221 °F
Styron DL 247A Plastic Pigment
Performance Features: Oil well, gas blocking, high temperature gas migration controlApplications: Modified ConcreteNorth AmericaInformation provided by Styron
Glass Transition Temp, Tg 105 °C
221 °F
Zeon Chemicals Zeonor® 1020R Cyclo-Olefin Polymer
Zeonor 1060R shall be in the form of pellets.
Glass Transition Temp, Tg 105 °C
221 °F
Ultimate Tg; TMA
Tra-Con Supertherm 826M01 High Performance Diamond Epoxy Adhesive
SUPERTHERM 826M01 is a one-part, smooth paste ULTRA HIGH THERMALLY CONDUCTIVE diamond filled epoxy adhesive recommended for semiconductor die-attach and other micro-electronic applications where the..
Glass Transition Temp, Tg 105 °C
221 °F
Ultimate Tg
Tra-Con Tra-Bond F118 Fiber Optic Epoxy Adhesive
TRA-BOND F118 is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows mor..
Glass Transition Temp, Tg 105 °C
221 °F
Ultimate Tg
Tra-Con Tra-Bond F118CLR Fiber Optic Epoxy Adhesive
TRA-BOND F118CLR is an impact resistant, fiber-optic adhesive designed for use in any optical connector. This two-part epoxy remains at a constant viscosity for a minimum of 30 minutes. This allows ..
Glass Transition Temp, Tg 105 °C
221 °F
Ultimate Tg
Tra-Con Tra-Duct 921M01 Low Viscosity Long Pot Life Silver-Filled Epoxy
TRA-DUCT 921M01 is a two component, silver-filled electrically conductive epoxy adhesive designed for applications which require electrical conductivity and a long pot life at a relatively low heat ..
Glass Transition Temp, Tg 105 °C
221 °F
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix
HexPly® M26 is an advance modified epoxy resin developed for aerospace and industrial markets. Its controlled flow, high peel strength on honeycomb cores and excellent fire behavior give it a cost ..
Glass Transition Temp, Tg 105 °C
221 °F
10°C/min test
Polimeri Europa SINKRAL D720 ABS, Impact Grade  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-08-35-15 High impact injection moulding grade, with improved flow compared with SINKRAL B620 and a high glo..
Glass Transition Temp, Tg 105 - 110 °C
221 - 230 °F
Average value: 107 °C Grade Count:3
Overview of materials for Acrylic, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate ..
Glass Transition Temp, Tg 105 °C
221 °F
10°C/min test
Polimeri Europa SINKRAL L320 ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-16-25 General purpose, high flow injection moulding grade having good impact resistance coupled with an ..