Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 78.0 - 80.0 °C | 172 - 176 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-109JS PET Sheet Grade Used mainly for 5 to 20 liter mineral water containers |
|||
Glass Transition Temp, Tg | 78.0 - 80.0 °C | 172 - 176 °F | PEPL-10-W-19 |
Pearl Engineering PEPLPET B-113C PET Sheet Grade Used mainly for box strapping. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | |
Eastman Eastapak 9921W PET
(discontinued **) Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 8007D-61 Cyclic Olefin Copolymer (COC) TOPAS® 8007D-61 is an externally lubricated version of our 8007 series of injection molding resins, targeting injection blow molding (IBM) and injection stretch blow molding (ISBM) applications. Li.. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 8007F-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and.. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | DSC |
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | Ultimate Tg |
Tra-Con Tra-Duct 2705 Room Temperature Conductive Nickel Epoxy Adhesive TRA-DUCT 2705 is an electrically conductive nickel filled epoxy adhesive recommended for electronic bonding, sealing, and EMI-RFI shielding applications. This two-part smooth paste formulation is fr.. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 8007F-400 Cyclic Olefin Copolymer (COC) TOPAS® 8007F-400 is a robust film extrusion grade designed for blending with polyethylene (PE). It is a moderate clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, .. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | |
Eastman Eastapak 9921 PET ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 1/MA/1/007 |
Dow LIGHTER™ C88 Polyethylene Terephthalate (PET) Resin LIGHTER™ resins are polyethylene terephthalate produced from PTA and MEG. These polymers are specifically designed for the production of beverage, food and other liquid containers and for thermofo.. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 1/MA/1/007 |
Dow LIGHTER™ C93 Polyethylene Terephthalate (PET) Resin LIGHTER™ resins are polyethylene terephthalate produced from PTA and MEG. These polymers are specifically designed for the production of beverage, food and other liquid containers and for thermofo.. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 1/MA/1/007 |
Dow LIGHTER™ C98 Polyethylene Terephthalate (PET) Resin LIGHTER™ resins are polyethylene terephthalate produced from PTA and MEG. These polymers are specifically designed for the production of beverage, food and other liquid containers and for thermofo.. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 1/MA/1/007 |
Dow LIGHTER™ S93 Polyethylene Terephthalate (PET) Resin LIGHTER™ S93 is a polyester polymer modified to improve infrared reheating of preforms. It provides very good mechanical properties and a wide processing range on all injection molding machines. .. |
|||
Glass Transition Temp, Tg | 78.0 °C | 172 °F | 1/MA/1/007 |
Dow LIGHTER™ S98 Polyethylene Terephthalate (PET) Resin LIGHTER™ S98 is a polyester polymer modified to improve infrared reheating of preforms. It provides very good mechanical properties and a wide processing range on all injection molding machines. .. |