Material Notes:
TOPAS® 8007D-61 is an externally lubricated version of our 8007 series of injection molding resins, targeting injection blow molding (IBM) and injection stretch blow molding (ISBM) applications. Like the rest of the 8007 series, 8007D-61 is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface making it an excellent choice for healthcare and food products. Lower leachables and extractables of TOPAS COC preserve food and drug stability and quality. Key applications and attributes: Drug delivery: Low leachables & extractables, low water transmission Prefilled syringes, vials, cartridges: Non-ionic, does not promote adsorption like glass Bottles and tubes: Minimally reactive, EtO and irradiation sterilizable Surgical instruments: Chemically resistant to alcohol, acetone, and acrylates IV containers and components: Transparent, withstands EtO and gamma sterilization Labware: Temperature resistance, clarity and purity Food packaging: Not manufactured with BPA, phthalates, or halogens Healthcare and food: Broad regulatory approval Information provided by TOPAS Advanced Polymers
Physical Properties Metric English Comments
Water Vapor Permeability 0.985 g mil/ (m2 day)
0.0635 g mil/ (100 in2 day)
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Water Absorption at Saturation 0.010 %

@Temperature 23.0 °C
0.010 %

@Temperature 73.4 °F
ISO 62
Water Vapor Transmission 0.0000250 g/m²/day

@Temperature 23.0 °C
0.00000161 g/100 in²/day

@Temperature 73.4 °F
85% RH; DIN 53122
Melt Flow 29.4 g/10 min

@Load 2.16 kg,
Temperature 260 °C
29.4 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.0 MPa
9140 psi
5mm/min; ISO 527-2/1A
Elongation at Yield 4.5 %
4.5 %
5mm/min; ISO 527-2/1A
Tensile Modulus 2.60 GPa
377 ksi
1mm/min; ISO 527-2/1A
Charpy Impact Unnotched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.260 J/cm²

@Temperature 23.0 °C
1.24 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ISO 75-1,-2
Vicat Softening Point 80.0 °C
176 °F
B50 (50°C/h 50N); ISO 306
Glass Transition Temp, Tg 78.0 °C
172 °F
10°C/min; ISO 11357-1,-2,-3
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Optical Properties Metric English Comments
Refractive Index 1.53
1.53
ISO 489
Transmission, Visible 91 %
91 %
ISO 13468-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
IEC 60093
Dielectric Constant 2.35

@Frequency 1000 - 10000 Hz
2.35

@Frequency 1000 - 10000 Hz
IEC 60250
Comparative Tracking Index >= 600 V
>= 600 V
IEC 60112