Material Notes:
TOPAS® 8007F-400 is a robust film extrusion grade designed for blending with polyethylene (PE). It is a moderate clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and general purpose applications. It is used in blends in both cast and blown processes, and in monolayer and multilayer products. Leading film applications include twist wrap, forming webs, protective packaging, shrink films and labels, and easy tear packaging. Industrial uses include thermoforming enhancement for PE and PP sheet products. Key applications and attributes: Forming films (header bags, etc.): Clarity, forming, barrier, purity, halogen-free Protective packaging: Stiffness for downgauging, improved forming Shrink films and labels: High shrink, low stress, gloss, toughness Twist films: Outstanding deadfold, clean cutting Decorative sheet: Stiffness, chemical resistance, forming, even draw Food packaging: Not manufactured with BPA, phthalates, or halogens Food contact: Broad regulatory approval Information provided by TOPAS Advanced Polymers
Physical Properties Metric English Comments
Oxygen Permeability 970 cm<sup>3</sup> mil/(m<sup>2</sup> day atm)
62.6 cm<sup>3</sup> mil/(100 in<sup>2</sup> day atm)
Water Vapor Permeability 3.70 g mil/ (m<sup>2</sup> day)
0.239 g mil/ (100 in<sup>2</sup> day)
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Water Absorption at Saturation 0.010 %
<br>@Temperature 23.0 °C
0.010 %
<br>@Temperature 73.4 °F
ISO 62
Thickness 70.0 microns
2.76 mil
Film
Melt Flow 1.8 g/10 min
<br>@Load 2.16 kg,<br> Temperature 190 °C
1.8 g/10 min
<br>@Load 4.76 lb,<br> Temperature 374 °F
ISO 1133
10.1 g/10 min
<br>@Load 2.16 kg,<br> Temperature 230 °C
10.1 g/10 min
<br>@Load 4.76 lb,<br> Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 3.4 %
3.4 %
ISO 527-3
Film Elongation at Break, TD 3.4 %
3.4 %
ISO 527-3
Tensile Modulus 1.70 GPa
247 ksi
Film, TD; ISO 527-3
2.10 GPa
305 ksi
Film, MD; ISO 527-3
Film Tensile Strength at Break, MD 55.0 MPa
7980 psi
ISO 527-3
Film Tensile Strength at Break, TD 50.0 MPa
7250 psi
ISO 527-3
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 78.0 °C
172 °F
10°C/min; ISO 11357-1,-2,-3
Descriptive Properties Value Comments
Type of film extrusion Cast