TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and healthcare applications. It is used in monolayer cast applications, and in coextrusion in both cast and blown processes, for a wide variety of film and sheet products requiring excellent optics in applications such as blister, twist, barrier, shrink and easy tear packaging. Industrial uses include formed decorative sheet products. Key applications and attributes: Pharmaceutical blisters: Clarity, forming, barrier, purity, halogen-free Deep draw barrier trays: Excellent deep draw, unlike other barriers Shrink films and labels: High shrink, low stress, gloss, clarity, toughness Twist films: High gloss, outstanding deadfold, clean cutting Decorative sheet: Gloss, hardness, chemical resistance, forming Food packaging: Not manufactured with BPA, phthalates, or halogens Information provided by TOPAS Advanced Polymers
Physical Properties Metric English Comments
Oxygen Permeability 977 cm3 mil/(m2 day atm)
63.0 cm3 mil/(100 in2 day atm)
Water Vapor Permeability 3.70 g mil/ (m2 day)
0.239 g mil/ (100 in2 day)
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Water Absorption at Saturation 0.010 %

@Temperature 23.0 °C
0.010 %

@Temperature 73.4 °F
ISO 62
Water Vapor Transmission 0.000800 g/m²/day

@Temperature 38.0 °C
0.0000515 g/100 in²/day

@Temperature 100 °F
90% RH; ISO 15106-3
Thickness 70.0 microns
2.76 mil
Film
Melt Flow 1.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 2.9 %
2.9 %
ISO 527-3
Film Elongation at Break, TD 3.0 %
3.0 %
ISO 527-3
Tensile Modulus 1.80 GPa
261 ksi
Film, TD; ISO 527-3
2.20 GPa
319 ksi
Film, MD; ISO 527-3
Elmendorf Tear Strength MD 225 g
225 g
ISO 6383-2
Elmendorf Tear Strength TD 230 g
230 g
ISO 6383-2
Dart Drop Test <= 36.0 g
<= 0.0794 lb
F50; ISO 7765-1
Film Tensile Strength at Break, MD 57.0 MPa
8270 psi
ISO 527-3
Film Tensile Strength at Break, TD 50.0 MPa
7250 psi
ISO 527-3
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 78.0 °C
172 °F
10°C/min; ISO 11357-1,-2,-3
Optical Properties Metric English Comments
Haze <= 1.0 %
<= 1.0 %
Film; ISO 14782
Gloss >= 100 %
>= 100 %
60°, Film; ISO 2813
Descriptive Properties Value Comments
Type of film extrusion Cast
Test specimen