Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -70.0 °C | -94.0 °F | |
Natural Rubber, Not Vulcanized (NR, IR, Polyisoprene) Natural rubber is polyisoprene. Chemical and environmental resistance and mechanical properties are improved through crosslinking (vulcanizing), usually through treatment with sulfur.Natural rubber.. |
|||
Glass Transition Temp, Tg | -70.0 °C | -94.0 °F | |
Styron XZ 92027.00 Carboxylated Butadiene Acrylate Performance Features: General purpose paper removable PSA, low adhesive transfer to paper and polyolefin substrates Applications: PSAEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -70.0 °C | -94.0 °F | DSC |
Lubrizol Estane® 58123 Thermoplastic Polyurethane Features: High moisture vapor transmission with low water swell and excellent low temperature and elasticity properties.Uses: Blown and flat die/cast film extrusion, injection molding and cable jack.. |
|||
Glass Transition Temp, Tg | -70.0 °C | -94.0 °F | DSC |
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el.. |
|||
Glass Transition Temp, Tg | -70.0 °C | -94.0 °F | ASTM D3418 |
DSM Biomedical BioSpan® F SPU Segmented Polyether Polyurethane (SPU) The flex life exhibited by BioSpan® SPU enables good performance in many different types of medical devices. This elastomeric polymer has shown the ability to withstand millions of flex cycles.The .. |
|||
Glass Transition Temp, Tg | -70.0 °C | -94.0 °F | |
3M Scotchcast™ 2104 Electrical Insulating Resin Scotchcast 2104 Electrical Insulating Resin is a hard, two-part, polyurethane resin encapsulant designed especially for permanent splice protection. 2104 is formulated for virtually every electrical.. |
|||
Glass Transition Temp, Tg | -70.0 °C | -94.0 °F | Cured property; JMTP 200 |
Aptek 2100-A7C/B Low modulus urethane staking compound APTEK 2100-A7C/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Althoug.. |
|||
Glass Transition Temp, Tg | -70.0 °C | -94.0 °F | Cured property; JMTP P-200 |
Aptek 2205 A/B Low modulus urethane stacking compound APTEK 2205-A/B is a thixotropic, two component, electrically insulating, low modulus urethane system designed for the staking of electrical/electronic components to printed circuit boards. Although.. |
|||
Glass Transition Temp, Tg | <= -70.0 °C | <= -94.0 °F | ASTM D746 |
Ashley Polymers Ashlene® 935-40M Nylon 11 A rotational molding grade Nylon 11 with a 40-50 mesh.Data provided by the manufacturer |
|||
Glass Transition Temp, Tg | -70.0 °C | -94.0 °F | Cured property; JMTP P-100 |
Aptek DAT-A-THERM 1000 Electrically insulating urethane film DAT-A-THERM 1000 is a tough, flexible, void free, electrically insulating urethane film designed to fill air gaps and dissipate heat between devices and substrates. DAT-A-THERM 1000 film is a 100% s.. |