Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman Aqua 20837 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 15041 PET
(discontinued **) Voridian polymer 15041 is a PET thermoplastic polyester.Applications/UsesCrystallized PET (CPET) trays |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 9663 PET
(discontinued **) VORIDIAN PET 9663 is a PET homopolymer widely used in the heatset industry and is FDA approved for food contact in hotfill applications. Voridian PET 9663 has a wide processing window and it’s vers.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 9921 PET Film
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 9921 PET Injection Molded
(discontinued **) VORIDIAN polymer 9921 is a copolymer PET that has been crystallized. Color concentrates of polymer 9921 are available on request.Applications/UsesAutomotive parts containersFood packagingHousehold p.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 9921P PET Film
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 9921P PET Injection Molded
(discontinued **) Voridian PET 9921P is produced at Voridian’s manufacturing sites in Rotterdam and Zarate, it is PTA/CHDM based, and it is sold to customers in the Europe, Middle East and Africa, Argentina, Bolivia.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman BD445 PET
(discontinued **) Voridian Polymer BD445 is primarily targeted for the soft drink and water markets, it is also suitable for use in other beverage containers as well as food and on-food-related applications. This pol.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman CA12 PET
(discontinued **) Voridian Polymer CA12 is currently produced to Voridian’s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer CA12 offers imp.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman CB12 PET
(discontinued **) Voridian CB12 polymer is a polyethylene terephthalate resin designed specifically for the carbonated soft drink (CSD) and other beverage markets. CB12 delivers fast, efficient processing and good ov.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
Americas Styrenics Styron® 685 Polystyrene
(discontinued **) STYRON® 685 general purpose polystyrene resin is a high heat resin used in consumer electronics and housewares. It offers excellent clarity, good moldability for use in hot runner systems. When use.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
Micropol Isoplas P651 Crosslinkable Polyethylene Information provided by Micropol Limited |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
Styron CALIBRE™ 891 20 Polycarbonate, General Purpose CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
Styron Pulse® 1550 ABS + Polycarbonate, 10% Glass Reinforced PULSE® 1550 Engineering resin is a 10% glass reinforced resin which offers a superior total performance with a balance of high heat resistance, practical toughness and ease of processing.Data pro.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
Borealis BorPEX™ ME2510 Medium Density Polyethylene Compound for Crosslinked Pipes (Pex-B (Silane)) BorPEX ME2510 is a silane crosslinkable compound which is used together with a catalyst masterbatch (Cat-MB) to accelerate the moisture-induced crosslinking reaction. It is designed for crosslinkab.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6 Zytel 73G45 BK263 is a 45% glass fiber reinforced black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
Hippe PA 11 Nylon 11 Water armatures, bearing under water, seals, housings, fans, insulated parts, parts for textile machines and household units. Toother wheels, sliding components and guides. Very low water absorpti.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
Hippe PA 12 Nylon 12 Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorptio.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
Hippe PA 46 Nylon 46 PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app.. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | |
Dow Tyril® 100 SAN Data provided by Dow Chemical. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 5214A PET
(discontinued **) Voridian PET 5214A is a bright and transparent amber homopolymer that meets light barrier requirements while maintaining the desirable attributes of PET. This resin is commonly used to mold containe.. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Specific Heat Capacity | 2.10 J/g-°C @Temperature 280 °C |
0.502 BTU/lb-°F @Temperature 536 °F |
ASTM E1269 |
Eastman 9921W PET Injection Molded
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |
|||
Specific Heat Capacity | 2.10 J/g-°C | 0.502 BTU/lb-°F | Average value: 2.10 J/g-°C Grade Count:3 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |