Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | Average value: 2.40 J/g-°C Grade Count:15 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | |
EVALCA EVAL® LC-L101A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 27 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, melt phase forming. Highest gas barrier EVOH available. EVOH is used in packaging applications because of its outstanding gas .. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | |
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | |
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | |
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | Estimated by MatWeb from similar grades |
EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applicat.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | |
EVALCA EVAL® LC-H101BD Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Blown film. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of th.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | |
EVALCA EVAL® K102 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 38 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | |
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, specialty applications. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now p.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | Estimated by MatWeb from similar grades |
EVALCA EVAL® G110 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a part of the Kuraray product line. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | Estimated by MatWeb from similar grades |
EVALCA EVAL® EF-XL Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) Biaxially oriented type film; property values for 15 µm film.Data provided by EVALCA. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produ.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | Estimated by MatWeb from similar grades |
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | Estimated by MatWeb from similar grades |
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc.. |
|||
Specific Heat Capacity | 2.40 J/g-°C | 0.574 BTU/lb-°F | Estimated by MatWeb from similar grades |
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr.. |