Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 3414R PC 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® 3414R PC (Asia Pacific) 40% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® FL930 PC Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® FL930 PC (Asia Pacific) Various weight reductions at 0.250"" (6.35 mm) wall, 30% GR. Superior flex strength/modulus, good tensile strength. V-0/5VA at 0.250"" (6.35 mm). |
|||
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | ASTM C351 |
SABIC Innovative Plastics Lexan® FL933 PC Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized. |
|||
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | |
Specialty Coating Systems Parylene HT® Poly (P-Xylylene) Coating Parylene HT is a polymer of para-xylylene with the alpha hydrogen atoms of the N dimer replaced with fluorine. This variant of Parylene is useful in high temperature applications (short term up to 4.. |
|||
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | |
Ensinger TECASINT 1011 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | |
Ensinger TECASINT 1101 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | |
Ensinger TECASINT 4011 Polyimide, Yellow (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Specific Heat Capacity | 1.04 J/g-°C | 0.249 BTU/lb-°F | Product Property; E1461-01 |
Arlon Thermabond® 48991A010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Description: Generation IIa Thermabond® NP electrically insulating electronic adhesive. Bonds without primer.Design/Construction: Liner: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style .. |