Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 327 °C | 621 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Fluorosint® 207 PTFE + mica, compression moulded (ISO Data) This material has a food contact compliant composition which, in combination with the good mechanical performance, dimensional stability, sliding and wear properties and inherent outstanding chemica.. |
|||
Melting Point | 327 °C | 621 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Melting Point | 327 °C | 621 °F | DSC, 10°C/min.; ISO 11357-1/-3 |
Quadrant EPP Semitron® ESd 500HR PTFE, static dissipative, extruded (ISO Data) Reinforced with a proprietary synthetic mica, Semitron ESd 500HR offers an excellent combination of low frictional properties, good dimensional stability and electrostatic dissipation. Whenever virg.. |
|||
Melting Point | 327 - 333 °C | 621 - 631 °F | |
Solvay Specialty Polymers Polymist® XPH-284 PTFE Powder Lubricant
(discontinued **) Meets the requirements of 21 CFR 177.1550.Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-u.. |
|||
Melting Point | 327 °C | 621 °F | Average value: 327 °C Grade Count:24 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Melting Point | 327 °C | 621 °F | Average value: 327 °C Grade Count:7 |
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum .. |
|||
Melting Point | 327 °C | 621 °F | Dry; DSC |
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation .. |
|||
Melting Point | 327 °C | 621 °F | ISO 11357-3 |
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran.. |
|||
Melting Point | 327 °C | 621 °F | DSC; ISO 3146 |
Solvay Specialty Polymers Amodel® HFZ A-4133L Polyphthalamide (PPA), 33% Glass Fiber Amodel® HFZ A-4133 L polyphthalamide (PPA) is a 33% glass-reinforced, hot water moldable resin. Key properties include heat resistance, reduced outgassing and high strength and stiffness over a b.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON M-18 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Suited to molding of large billets, has nearly the same molding characteristics of M-12. Also allows uniform mixing of inorganic fi.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON M-391 PTFE Molding Powder, Free Flow Free flow powder.Processing Methods: Compression molding and automatic or semi-automatic compression molding.Features: Used if concerned about insufficient molding pressure for flat sheets.Informati.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON MG-1050F PTFE 25% Glass Fiber Filled Molding Powder, High Apparent Density, Free Flow 25% glass fiber filled. High apparent density and free-flowing properties. High wear resistance, low friction, good electrical properties.Applications: Mechanical and electrical service. Availabl.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON MG-1241 PTFE 20% Glass Fiber and 5% Graphite Filled Molding Powder 20% glass fiber and 5% graphite filled. High wear resistance, low friction, high creep resistance.Applications: Mechanical and chemical service (e.g. piston rings, bearing pads, and packings)Inform.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON MG-2030 PTFE 15% Graphite Filled Molding Powder 15% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON MG-2060 PTFE 30% Graphite Filled Molding Powder 30% graphite filled. Low friction, excellent chemical resistance, high creep resistance.Applications: Mechanical and chemical service (e.g. bearings, gaskets, packings)Information provided by Daiki.. |
|||
Melting Point | 327 °C | 621 °F | |
Daikin POLYFLON MG-6030F PTFE 15% Carbon Fiber Filled Molding Powder, High Apparent Density, Free Flow 15% carbon fiber filled. High apparent density and free-flowing properties. High wear resistance, high load resistance, high bend resistance.Applications: Mechanical service (e.g. bearings, mechan.. |
|||
Melting Point | 327 °C | 621 °F | |
Azoty Tarnow™ TARFLEN SG-1 PTFE Free-Flowing suspension powder for automated compression molding of complicated shapes and isostatic pressing.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 125 PTFE, 35% Carbon Filled Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | |
Azoty Tarnow™ TARFLEN SM-K25 PTFE Based on Tarflen SM1 reinforced with 25% coke for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 139 PTFE, 35% Soft Carbon Filled Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 206 PTFE, 15/5% Glass/MoS2 Filled Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 209 PTFE, 15% Glass Filled Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 451 PTFE, organic filler Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | DSC |
Adamas Adalon® 704 PTFE, Long Carbon Fiber Information provided by Adamas, HPM |
|||
Melting Point | 327 °C | 621 °F | ASTM D3418 |
Quadrant EPP Semitron® ESd 500 HR PTFE, static dissipative, compression molded (ASTM Product Data Sheet) |