Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 295 °C | 563 °F | STN EN 11357-1 |
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved.. |
|||
Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
DSM Stanyl® 46HF5050 (DAM) Nylon 46 50% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TE250F9 Nylon 46-45% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TE341 Nylon 46 (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TE351 PA46 FR(17) Flame Retardant, Heat Stabilized |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TS250F8 PA46-GF40 FR 40% Glass Reinforced, Flame Retardant, Heat Stabilized |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TS256F8 Nylon 46-40% Glass Reinforced (Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TW200B6 PA46-CF30 30% Carbon Reinforced, Heat Stabilized, Lubricated |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TW271F6J10 (PA46+PTFE)-GF30 30% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
DSM Stanyl® TW275F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Molydisulfide Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
DSM Stanyl® TW300 (COND) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
DSM Stanyl® TW300 (DAM) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
DSM Stanyl® TW341 (COND) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
DSM Stanyl® TW441 (COND) Nylon 46 High Viscosity, Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
DSM Stanyl® TW441 (DAM) Nylon 46 High Viscosity, Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30 Product description: Grivory XE 4027 black 9916 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semicrystalline, partially aromatic copolyam.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4355 G5 25% Glass Filled PA6/6T (Dry) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4357 G6 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4357 G6 BK 00564 30% Glass Filled PA6/6T (Dry) Description: 30% glass-fiber reinforced, impact-modified product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechan.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TE350 Nylon 46 (European and Asian Grade) (Cond)
(discontinued **) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TE250F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TS256F6 Nylon 46-30% Glass Reinforced (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |