Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 285 °C | 545 °F | |
Chevron Phillips Ryton® A-200 PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Melting Point | 285 °C | 545 °F | |
Chevron Phillips Ryton® R10 5002C PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Melting Point | 285 °C | 545 °F | |
Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
Melting Point | 285 °C | 545 °F | ISO 11357-3 |
Solvay Specialty Polymers Ryton® QC200N Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
Melting Point | 285 °C | 545 °F | ISO 11357-3 |
Solvay Specialty Polymers Ryton® QC220P Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
Melting Point | 285 °C | 545 °F | |
ScanTube MFA Tubing Information provided by ScanTube, Inc. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON C2040G5 PPS, cross-linked, 40% GF, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON C2065X3 PPS, cross-linked, 65% glass fiber / mineral reinforced, reduced residual chlorine PPS-GF/MD 65Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON L1040G3 PPS, linear, 40% glass fiber reinforced PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATRON L2040G3 PPS, linear, 40% glass fiber reinforced, reduced residual chlorine PPS-GF40Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 285 °C | 545 °F | |
Chevron Phillips Ryton® R-4 04 PPS (Polyphenylene Sulfide)
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |