Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Nylene® PA6/6 Impact Modified 4120 HS Nylon 6/6; MoS2 lube
High Impact Grade; Property data for dry as molded samples.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Melting Point 252 °C
486 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Rynite® FR530L BK507 PET  (Unverified Data**)
Rynite® FR530L BK507 is a 30% glass reinforced, flame retardant, modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Melting Point <= 252 °C
<= 486 °F
Invista Polyclear® Conserve™ 1101D PET Copolymer Packaging Resin  (discontinued **)
Polyclear® Conserve™ PET 1101D is a copolymer packaging resin containing 20% post consumer recycled PET. It has a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Conserve..
Melting Point <= 252 °C
<= 486 °F
Invista Polyclear® Conserve™ 1101F PET Copolymer Packaging Resin  (discontinued **)
Polyclear® Conserve™ PET 1101F is a copolymer packaging resin containing 10% post consumer recycled PET. It has a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Conserve..
Melting Point <= 252 °C
<= 486 °F
DSC test
Invista 2201U Copolymer Packaging Resin  (discontinued **)
Carboxyl end groups:
Melting Point 252 - 275 °C
486 - 527 °F
Average value: 258 °C Grade Count:50
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Melting Point 252 - 295 °C
486 - 563 °F
Indium Corp. Indalloy 157 Lead Solder Alloy
Information Provided by Indium Corporation
Melting Point 252 - 258 °C
486 - 496 °F
DSC
Iran Petrochemical (PCC) TG 621 Polyethylene Terephthalate
Polyethylene Terephthalate fiber grade chips, semi dullApplications: staple fiber, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co.
Melting Point <= 252 °C
<= 486 °F
Peak Melting Point; ExxonMobil method
ExxonMobil Exceed™ 1327HA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1327HA is a metallocene ethylene-hexene copolymer. Films made from Exceed 1327HA resin have excellent tensile, impact strength and puncture. These superior strength prope..
Melting Point <= 252 °C
<= 486 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LLDPE LL 4004EL Wire & Cable Linear Low Density Polyethylene Resin (European Grade)
Product Description: LL 4004EL is a C4 Ziegler Natta LLDPE, especially designed for Low Voltage power cable insulation, using the two-step silane cross-linking process. Sufficient Cu-inhibitor shoul..
Melting Point <= 252 °C
<= 486 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LLDPE LL 5001.09 Linear Low Density Polyethylene Resin
Product Description: LL 5100.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular from of LL 5100.09 makes for efficient blending ..
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 525-13G Nylon 66, 13% Glass Reinforced
High impact Nylon 66 reinforced with 13% glass fibers.Data provided by the manufacturer
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 527-13G Nylon 66, 13% Glass Reinforced
A 13% glass reinforced, impact modified Nylon 66.Data provided by the manufacturer
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 527-25G Nylon 66, 25% Glass Reinforced
A 25% glass reinforced impact modified Nylon 66.Data provided by the manufacturer
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 527-43G Nylon 66, 43% Glass Reinforced
A 43% glass reinforced impact modified Nylon 66.Data provided by the manufacturer
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 527LD-33G Nylon 66, High Impact, 33% Glass Reinforced
A high impact reinforced Nylon 66 with good low temperature properties.Data provided by the manufacturer
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 527LD-45LG Nylon 66, 45% Long Glass Fiber Reinforced
Long glass fiber reinforced impact modified Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced r..
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 528L2 Nylon 66
A general purpose highly lubricated Nylon 66 resin.Data provided by the manufacturer
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 528L-30G Nylon 66, 30% Glass Reinforced
General purpose glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufacture..
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 528L-5G Nylon 66, 5% Glass Reinforced
General purpose glass fiber reinforced nylon, designed for parts requiring improved dimensional stability and higher strength than conventional resins.Data provided by the manufacturer
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 528LSB2-20G Nylon 66, 20% Glass Reinforced
A UV Stabilized 20% glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufac..
Melting Point 252 °C
486 °F
ASTM D789
Chem Polymer Chemlon 100 W Nylon 66, MoS2 Filled
A molybdenum disulfide modified nylon 66 exhibiting superior tensile strength and wear resistance, greater dimensional stability and higher heat resistance than general purpose nylon 66.Data provide..
Melting Point 252 °C
486 °F
ASTM D789
Chem Polymer Chemlon 182 Nylon 66, Flame Retarded
A non-halogenated, unfilled nylon 66 used in electrical applications where improved flame retardancy is required. The material has excellent moldability, good snap-fit properties and is available i..
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 520-25G Nylon 66, 25% Glass Reinforced
Nylon 66, 25% glass reinforced.Data provided by the manufacturer
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 520-33G Nylon 66, 33% Glass Reinforced
Nylon 66, 33% glass reinforced resin. Also available with Heat Stabilized and/or UV Stabilized.Data provided by the manufacturer
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 520-40G Nylon 66, 40% Glass Reinforced
A general purpose 40% glass reinforced Nylon 66 resin.Data provided by the manufacturer
Melting Point 252 °C
486 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Rynite FR530 BK507 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont Performance Polymers
Melting Point 252 °C
486 °F
ASTM D3418
Ashley Polymers Ashlene® 528SMS-30GB Nylon 66, 30% Glass Reinforced
A 30% glass reinforced, heat stabilized, black Nylon 66 with Molybdenum disulfide.Data provided by the manufacturer
Melting Point 252 °C
486 °F
10°C/min; ISO 11357-1/-3
DuPont Performance Polymers Rynite® 530HTE NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
30% Glass Reinforced Polyethylene Terephthalate with Excellent High Temperature Dielectric PropertiesRynite 530HTE NC010 is a 30% glass reinforced modified polyethylene terephthalate resin with exce..
Melting Point <= 252 °C
<= 486 °F
DSC test
Invista 1101R Copolymer Packaging Resin  (discontinued **)
Carboxyl end groups: