Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 225 °C | 437 °F | ISO 11357-1-3 |
Radici Raditer® B RV 150 Polybutylene Terephthalate with 15% Glass fiber Raditer® B RV 150 is a glass fiber reinforced thermoplastic polyester based on polybutylene terephthalate. The PBT compounds combine excellent thermal, mechanical, electrical and chemical properti.. |
|||
Melting Point | 225 °C | 437 °F | |
Eastman Eastar DN102 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melting Point | 225 °C | 437 °F | Peak at Break |
LG Chemical LUMAX GP5306F PBT+ABS+GF30%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF30%, Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 and 1309-64-4Information provided by LG .. |
|||
Melting Point | 225 °C | 437 °F | @ Break; ASTM D3418 |
LG Chemical Lupox® GP1000D PBT Description: Injection Molding, PBT, General PurposeApplication: Automotive (Head Lamp Bezel)CAS No. 30965-26-5Information provided by LG Chemical |
|||
Melting Point | 225 °C | 437 °F | @ Break; ASTM D3418 |
LG Chemical Lupox® SG3250 PBT+PET+MF25% Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Melting Point | 225 °C | 437 °F | ASTM D3418 |
A. Schulman SCHULADUR® A GB20 20% Glass Bead Reinforced PBT Information provided by A. Schulman. |
|||
Melting Point | 225 °C | 437 °F | ASTM D3418 |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Melting Point | 225 °C | 437 °F | |
Polyram RamSter RF300G4 PBT, 20% Glass Fiber 20% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Melting Point | 225 °C | 437 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnite® TV4 261 PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Melting Point | 225 °C | 437 °F | ASTM D3428 |
CRG Industries Essemplex AB43 Thermoplastic Shape Memory Polymer Resin Essemplex is a melt-processible shape memory polymer (SMP) resin. Its unique properties offer versatile design options for reconfiable and customizable products. Essemplex is compatible with current.. |
|||
Melting Point | 225 °C | 437 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Melting Point | 225 - 250 °C | 437 - 482 °F | 10 K/min; ISO 3146 |
Eurotec® Tecodur® PB70 GR20 NL CA 01 PBT/PET 20% glass fiber reinforced Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Melting Point | 225 °C | 437 °F | 10°C/min; ISO 11357-1/-3 |
Barlog Plastics KEBATER A9030 PBT, 30% glass fiber reinforced, improved surface quality, reduced warpage (PBT+X)-GF30Information provided by BARLOG plastics GmbH. |
|||
Melting Point | 225 °C | 437 °F | DIN EN 11357-1 |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Melting Point | 225 °C | 437 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Crastin® HR5330HF BK503 PBT
(Unverified Data**) Crastin® HR5330HF is a 30% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |
|||
Melting Point | 225 °C | 437 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnite® T06 202 XL (T-X01151) PBT (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Melting Point | 225 °C | 437 °F | |
Radici Radiflam® B RV250AE Polybutylene Terephthalate - 25% Glass fiber reinforced Radiflam® B is a range of flame retardant polybutylene terephthalate (PBT) used for injection molding and extrusion for all applications where high fire resistance is required.Information provided .. |