Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBATER A9030 PBT, 30% glass fiber reinforced, improved surface quality, reduced warpage

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled
Manufacturer Barlog Plastics
Trade Name KEBATER
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBATER A9030 PBT, 30% glass fiber reinforced, improved surface quality, reduced warpage.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
(PBT+X)-GF30Information provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.15 %
0.15 %
similar to ISO 62 test
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
ISO 527-1
Elongation at Break 2.5 %
2.5 %
ISO 527-1
Tensile Modulus 10.5 GPa
1520 ksi
ISO 527-1
Charpy Impact Unnotched 6.60 J/cm²
31.4 ft-lb/in²
ISO 179-1eU
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 225 °C
437 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
ISO 75-1/-2
Flammability, UL94 HB

@Thickness 0.800 mm
HB

@Thickness 0.0315 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Descriptive Properties Value Comments
Resin Type (PBT+X)-GF30