Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 220 °C | 428 °F | STN EN 11357-1 |
Plastcom PLASTAMID® 6 GF 20 002 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 20% glass fiber, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric hand tools, hobby tools, .. |
|||
Melting Point | 220 °C | 428 °F | |
Plastcom SLOVAMID 6 FRM 2 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Melting Point | 220 °C | 428 °F | STN EN 11357-1 |
Plastcom SLOVAMID® 6 GF 40 HI PA6 reinforced with glass fiber, improved impact strength PA 6 for injection molding, reinforced with 40% glass fiber, impact modified. Application: impacted moldings and moldings with higher strength applied in automotive, electrical, engineering and cons.. |
|||
Melting Point | 220 °C | 428 °F | |
Polimersan Plastics POLIPA® (PA 6) Polyamide POLIPA® PA6 (POLYAMIDE) is produced by poly condensation of e-aminoacid and by the help of d-carbon acid and d-amine poly condensation. Its characteristics depend upon the numbers of the main struc.. |
|||
Melting Point | 220 °C | 428 °F | ISO 11357-3 |
Pasargad Polymer Peyvand Pasamid 3P-H1130B Nylon 6, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Melting Point | 220 °C | 428 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Akulon® Ultraflow™ K-FG12 Nylon 6-60% Glass Reinforced (European Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Melting Point | 220 - 325 °C | 428 - 617 °F | Average value: 267 °C Grade Count:25 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Melting Point | 220 °C | 428 °F | ASTM and ISO test |
BASF Capron® 8200 HS BK-102 Nylon 6 (Dry)
(discontinued **) Capron 8200 HS BK-102 is a medium viscosity, heat stabilized, pigmented black, nylon 6 injection molding homopolymer exhibiting resistance to sink-mark formation in thick section, and improved tough.. |
|||
Melting Point | 220 °C | 428 °F | ASTM and ISO test |
BASF Capron® 8200CQ Blend Nylon 6 (Dry)
(discontinued **) Capron 8200CQ Blend is a medium viscosity, nylon 6 injection molding homopolymer possessing the combination of strength, stiffness and toughness properties as well as chemical and abrasion resistanc.. |
|||
Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
Gromax BFG30-FN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
Gromax BFG45-DN00N1 Nylon 6 46% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melting Point | 220 °C | 428 °F | DIN EN ISO 314 |
GEHR Plastics PA 6 C Nylon 6 Cast Very stressed-relieved and high-molecular weight PA6.Temperature resistant from -40° to approx. 100°C and high stiffness, hardness and toughness. The good mechanical characteristics will be ac.. |
|||
Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1,-3 |
Gromax BFG30-FH00B2 Nylon 6 30% Glass Filled (Conditioned) Information provided by Gromax Enterprises Corp. |
|||
Melting Point | 220 °C | 428 °F | ISO 3146 |
Wellman Wellamid® MRGF25/15 42H-N2/WE1705-N2 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced Improved surface appearance gradeAll information provided by Wellman Engineered Resins. |
|||
Melting Point | 220 °C | 428 °F | 10°C/min; ISO 11357-1/-3 |
DSM Akulon® F249-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Melting Point | 220 °C | 428 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Akulon® K224-G6 (Cond.) 30% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Melting Point | 220 °C | 428 °F | |
EMS-Griltech Grilon® BN 19 Nylon 6 Monofilament (Non-Set) Description: GRILON BN 19 is a Nylon 6 based monofilament for filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® S 4090 GM11 5/5% Glass/Mineral Filled PBT Description: Is a PBT + ASA, injection-molding grades reinforced with 5% glass fiber/mineral, for laminar parts with high demands on dimensional stability and low warpage, e.g. lids, ventilation gri.. |
|||
Melting Point | 220 °C | 428 °F | ASTM Test |
BASF Ultramid® 8202C PA6 (Conditioned) Ultramid 8202C is a modified crystalline and low viscosity, nylon 6 injection molding homopolymer. It is also available in heat stabilized (Ultamid 8202C HS) and/or pigmented versions. Its unique .. |
|||
Melting Point | 220 °C | 428 °F | 10 K/min |
BASF Ultramid® 8202CQ PA6 (Conditioned) Ultramid 8202CQ is a low viscosity, PA6 injection molding homopolymer, possessing a modified crystalline structure or increased property performance and faster cycles. It is also available in pigme.. |
|||
Melting Point | 220 °C | 428 °F | 10 K/min |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Melting Point | 220 °C | 428 °F | ISO 11357-1/-3 |
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Conditioned) Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF |
|||
Melting Point | 220 °C | 428 °F | ISO 3146 |
BASF Ultramid® B3UG4 Grey 22975 20% Glass Filled PA66 FR (Conditioned) Description: Halogen-free and phosphorus free flame retardant injection-molding grade with outstanding free-flow properties, good electrical properties and low smoke density; resistant to glow wire.. |
|||
Melting Point | 220 °C | 428 °F | 10K/min; ISO 3146 |
CENTROPLAST CENTROMID 6 E Polyamide 6 extruded This tough and impact resistant material has good chemical resistance and can be bonded and welded. It is used for sealing rings, flanges, etc. Information provided by CENTROPLAST Engineering Plast.. |
|||
Melting Point | 220 °C | 428 °F | ISO 11357-1/3 |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Melting Point | 220 °C | 428 °F | ISO 3146 |
BASF Ultramid® B3GM35 BK 60564 40% Glass/Mineral Filled PA6 (Dry) Description: Ultramid B3GM35 BK60564 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade.Applications: industrial articles requiring medium rigidity and.. |
|||
Melting Point | 220 °C | 428 °F | ASTM Test |
BASF Ultramid® TG7S 35% Glass Filled PA6 (Dry) Ultramid TG7S is a 34% glass reinforced, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the first North American seat
cushion .. |
|||
Melting Point | 220 °C | 428 °F | ISO 3146/C2 |
Addiplast Addinyl B2 ZM30 Nylon 6, 30% Mineral Filled Mineral filled, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Melting Point | 220 °C | 428 °F | DIN 53765 |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |