Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 179 °C | 354 °F | Masterbatch; ISO 11357-1,-3 |
Nanocyl PLASTICYL™ PA1502 Polyamide 12 with Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Melting Point | 179 - 232 °C | 354 - 450 °F | |
Indium Corp. Indalloy 127 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 179 - 260 °C | 354 - 500 °F | |
Indium Corp. Indalloy 142 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 179 - 289 °C | 354 - 552 °F | |
Indium Corp. Indalloy 154 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 179 - 253 °C | 354 - 487 °F | |
Indium Corp. Indalloy 210 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 179 - 179 °C | 354 - 354 °F | |
Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy Good general purpose solder. Can be used on silver bearing surfaces to reduce scavenging.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 179 °C | 354 °F | |
Heatbath/Park Aus-Quench Quenching and Tempering Salt Quench salt whose melting point and working range make it particularly suitable for ausquenching/austempering. (350 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Melting Point | 179 °C | 354 °F | |
Heatbath/Park Partherm 350 Heat Transfer Salt A lower cost alternative to Partherm 290 at some sacrifice in working range. (350 Parkettes)Information provided by Heatbath Corporation - Park Metallurgical. |
|||
Melting Point | 179 °C | 354 °F | Eutectic |
Indium Corp. Indalloy 104 Tin-Lead Solder Alloy Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation |
|||
Melting Point | 179 - 189 °C | 354 - 372 °F | |
Indium Corp. Indalloy 137 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 179 °C | 354 °F | |
Williams Advanced Alloys WS179 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Melting Point | 179 °C | 354 °F | DSC |
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Melting Point | 179 °C | 354 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
Melting Point | 179 °C | 354 °F | DIN 53 736 |
Hippe PA 12 Nylon 12 Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorptio.. |
|||
Melting Point | 179 °C | 354 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® RS LC1201 BK040A Nylon 1010
(Unverified Data**) Toughened Renewably Sourced Medium Viscosity Polyamide 1010 Developed for Extrusion Zytel RS LC1201 BK040A is a renewably sourced polyamide 1010 resin containing a minimum of 85% renewably sourced i.. |
|||
Melting Point | 179 °C | 354 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® L 25 Z PA12-I Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit.. |
|||
Melting Point | 179 °C | 354 °F | |
AIM 62Sn/Pb36/Ag2 Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 179 °C | 354 °F | ASTM D3418 |
Ashley Polymers Ashlene® D925LH-30G Nylon 12, 30% Glass Reinforced, Lubricated A 30% glass reinforced lubricated heat and light stabilized Nylon 12. Options: D925L-30G injection molding grade, without heat and light stabilizer; and D925L-30GB for injection molding, general pu.. |