Thermal Properties Metric English Comments
Melting Point 119 °C
246 °F
Internal method
Polimeri Europa Clearflex® H&T LFH 208 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T LFH 208 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LFH..
Melting Point 119 °C
246 °F
Internal method
Polimeri Europa Clearflex® H&T LFH 238 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T LFH 238 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion. It contains slip and antiblocking a..
Melting Point 119 °C
246 °F
Internal method
Polimeri Europa Flexirene® MS 40 A Linear Low Density Polyethylene
Flexirene MS 40 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 40 A are characterized by a good balance be..
Melting Point 119 °C
246 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin  (discontinued **)
Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength ..
Melting Point 119 °C
246 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Exceed™ 1518EC Tough Premium Film Resin  (discontinued **)
Exceed 1518EC resin is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1518EC resin have outstanding tensile, impact strength and puncture. These superi..
Melting Point 119 °C
246 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Exceed™ 1018 DA Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
Melting Point 119 °C
246 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Exceed™ 1018 FA Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
Melting Point 119 °C
246 °F
Exxon Method
ExxonMobil Exceed™ 350D60 LDPE/Hexene Tough Premium Film Resin  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 350D60 resin have outstanding tensile, impact streng..
Melting Point 119 °C
246 °F
DSC; ASTM D3418
DuPont Bynel® 41E623 Adhesive Resin  (discontinued **)
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Melting Point 119 - 139 °C
246 - 282 °F
TMA Melt Range
Huntsman IROGRAN® PS455-203 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Melting Point 119 °C
246 °F
UBE method
UBE UMERIT 2500F Metallocene LLDPE
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert..
Melting Point 119 °C
246 °F
DSC; ASTM D3418
DuPont Bynel® 41E687 Adhesive Resin
Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design..
Melting Point 119 °C
246 °F
DSC
Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin
TOTAL Petrochemicals Polypropylene LX5 02-15 is an experimental grade of isostatic polypropylene copolymer produced via TOTAL proprietary metallocene catalyst technology.Benefits. LX5 02-15 produc..
Melting Point 119 °C
246 °F
ISO 11357
Total Lumicene® mPE M 2735 S01 Metallocene Polyethylene, Cast Film
Lumicene® mPE M 2735 S01 is a Lumicene® metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 2735 S01 can be processed at high output rates with low extrusion pressure, low nec..
Melting Point 119 °C
246 °F
ASTM D3418, ISO 3146
DuPont™ Fusabond® E589 Polymer Modifier
DuPont™ Fusabond® E589 is an anhydride modified polyethylene. Uses: Adhesives Pipe Coating Tie-Layer Features premium adhesive for Pipe Coating tie-layer at high surface temperatures. ( 90°C)
Melting Point 119 °C
246 °F
Dow Method (DSC)
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin
DOW DNDA-7340 NT 7 LLDPE resin is well-suited for use in blow molding applications such as small, squeezable bottles, as well as, extruded flexible hoses and tubing. DOW DMDA-7340 NT 7 resin is als..
Melting Point 119 °C
246 °F
Dow Method (DSC)
Dow FLEXOMER™ DFDB-9042 NT Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDB-9042 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It has value as a sealant layer in multilayer film structures for dry and liquid packaging. I..
Melting Point 119 °C
246 °F
Dow Method (DSC)
Dow FLEXOMER™ GRSN-1539 NT 7 Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ GRSN-1539 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins ..
Melting Point 119 °C
246 °F
Dow Method (DSC)
Dow FLEXOMER™ DFDA-1010 NT 7 Very Low Density Polyethylene (VLDPE) Resin
FLEXOMER™ DFDA-1010 NT 7 is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins ..
Melting Point 119 °C
246 °F
DSC
Arkema Group OREVAC® 18370 Maleic Anhydride Modified Polyethylene
OREVAC® 18370 is anhydride modified polyethylene. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. OREVAC® 1..
Melting Point 119 °C
246 °F
Recrystallizing temperature; ISO 3146
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This..
Melting Point 119 °C
246 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Exceed™ 1018 EA Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
Melting Point 119 °C
246 °F
ISO 11357
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Blown Film
Lumicene® mPE M 2710 EP is a second generation metallocene based Low Density Polyethylene with hexene as comonomer.Lumicene® mPE M 2710 EP can be processed at high output rates with low extrusion ..
Melting Point 119 °C
246 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Exceed™ 1018 EB Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..
Melting Point 119 - 170 °C
246 - 338 °F
Average value: 154 °C Grade Count:73