Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 93.0 °C | 199 °F | Internal Method |
Polimeri Europa Greenflex® FC 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FC 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FC 45 exhibit good optical properties, excellent impact resistance and low creep.. |
|||
Melting Point | 93.0 °C | 199 °F | Internal Method |
Polimeri Europa Greenflex® FF 45 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion Greenflex FF 45 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FF 45 show high toughness.Main Applications: Greenflex FF 45 is recommended for.. |
|||
Melting Point | 93.0 °C | 199 °F | Freezing Point via DSC/ASTM D3418 |
DuPont 20 Series 2020 Specialty Polyethylene Resin
(discontinued **) DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc.. |
|||
Melting Point | 93.0 °C | 199 °F | DSC; ASTM D3418 |
DuPont Appeel® LSR11N704 Lidding Sealant Resin
(discontinued **) Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal.. |
|||
Melting Point | 93.0 °C | 199 °F | DSC; ASTM D3418 |
DuPont Appeel® LSR11D704 Lidding Sealant Resin
(discontinued **) Appeel® LSR11D704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable s.. |
|||
Melting Point | 93.0 °C | 199 °F | DTA |
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Melting Point | 93.0 - 99.0 °C | 199 - 210 °F | |
Indium Corp. Indalloy 40 Bismuth Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 93.0 - 127 °C | 199 - 261 °F | |
Indium Corp. Indalloy 68 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 93.0 °C | 199 °F | Eutectic |
Indium Corp. Indalloy® 8 In-Sn-Cd Fusible Alloy General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 93.0 °C | 199 °F | Freezing Point via DSC/ASTM D3418 |
DuPont 20 Series 2020T Specialty Polyethylene Resin DuPont 2020T and 2020 specialty low density polyethylene resins are products characterized by low melt index and intermediate crystallinity. These products, produced via a unique polymerization proc.. |
|||
Melting Point | 93.0 °C | 199 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 21E830 Anhydride Modified Ethylene Acrylate BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i.. |
|||
Melting Point | 93.0 °C | 199 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 22E804 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Melting Point | 93.0 °C | 199 °F | Freezing Point; ASTM D3418 |
DuPont™ Fusabond® P353 Polymer Modifier DuPont Fusabond® P353 is a chemically modified polypropylene. Uses: Automotive Applications Plastics Modification Polymer Modifier Applications: Coupling agent Long glass fiber filled PP compoun.. |
|||
Melting Point | 93.0 °C | 199 °F | ASTM D3418, ISO 3146 |
DuPont™ Surlyn® 8528 Sodium Ionomer Surlyn® 8528 is a sodium ionomer thermoplastic resin. It is available for use in conventional extrusion and injection equipment, to create various sheets or shapes. Surlyn® 8528 thermoplastic resi.. |
|||
Melting Point | 93.0 °C | 199 °F | DSC, 10°C/min (peak); DuPont Test |
Dow Engage® ENR 7086.01 Ethylene-Butene Copolymer Description: ENR 7086.01 is a revolutionary new ethylene-butene copolymer with a broader molecular weight distribution and much higher levels of long chain branching than other commercially availabl.. |
|||
Melting Point | 93.0 °C | 199 °F | 10°C/min |
Arkema Group Evatane® 1003 VL 4C Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Melting Point | 93.0 °C | 199 °F | 10°C/min |
Arkema Group Evatane® 1003 VL 4S Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Grade for transparent and thermal agricultural film to 180 at 200 µ for greenhouse coverage.ISO data prov.. |
|||
Melting Point | 93.0 °C | 199 °F | 10°C/min |
Arkema Group Evatane® 1003 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for transparent and thermal agricultural film for greenhouse coverage.ISO data provided by the manufacturer, Arkema. |
|||
Melting Point | 93.0 °C | 199 °F | 10°C/min |
Arkema Group Evatane® 1004 VL 4E Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the .. |
|||
Melting Point | 93.0 °C | 199 °F | DSC |
Arkema Group OREVAC® 9307 Y EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Melting Point | 93.0 °C | 199 °F | 10°C/min |
Arkema Group Evatane® 1005 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and very high mechanical properties. Examples: high strength stretch film, greenhous.. |
|||
Melting Point | 93.0 °C | 199 °F | DSC; ASTM D3418 |
DuPont™ Surlyn® 1702 Zinc Ionomer Resin for Extrusion Coating Surlyn® 1702 is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceutical.. |
|||
Melting Point | 93.0 °C | 199 °F | by DSC; ASTM D3418 |
Westlake EMAC® Plus SP1330 22% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® Plus SP1330 is a 22% EMA copolymer designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal temperatures are required. SP1330 is.. |
|||
Melting Point | 93.0 °C | 199 °F | DSC |
Arkema Group LOTRYL® 17 BA 04 Copolymer Ethylene - Butyl Acrylate LOTRYL® 17 BA 04 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 17 BA 04 is used as tie layer in coextrusion PP/PE, for extrusi.. |
|||
Melting Point | 93.0 °C | 199 °F | ASTM D3417- ISO 3146 |
DuPont Surlyn® 1702SBR
(discontinued **) DuPont™ Surlyn® 1702SBR is a zinc-type resin made from ethylene/methacrylic acid copolymer. This resin has slip, antiblock, and chill roll release additives included in the resin to reduce the coe.. |