Arkema Group Evatane® 1003 VL 4C Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer Arkema
Trade Name Evatane®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Arkema Group Evatane® 1003 VL 4C Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
EVA copolymer made by high pressure tubular process. Anti-UV stabilized grade. Applications Thermal and colorless agricultural film to 180 at 200 µ for greenhouse coverage.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
Melt Flow 0.45 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 7.00 MPa
1020 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.100 GPa
14.5 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 93.0 °C
199 °F
10°C/min
Vicat Softening Point 74.0 °C
165 °F
50°C/hr; 50N