Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 223 - 225 °C | 433 - 437 °F | |
Plastcom SLOVASTER® B/A GF 30 PBT, 30% glass fibre FeaturesPBT/ASA for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Melting Point | 200 - 225 °C | 392 - 437 °F | Average value: 223 °C Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | Average value: 220 °C Grade Count:61 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Melting Point | 221 - 225 °C | 430 - 437 °F | |
Johnson Matthey Plumbsol Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | |
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | |
Tisan TISLAMID® 6 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | |
Zig Sheng Industrial ZISAMIDE® HP1101 Nylon 6 ZISAMIDE® HP1101 is a spinning grade Polyamide 6. Application: textile semidullInformation provided by ZIG SHEN Industrial Co., LTD. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | |
BASF Ultradur B 4040 G6 High Speed BK15029 30% Glass Filled PBT/PET Ultradur B 4040 G6 High Speed BK15029 is a high flow, fast cycling with low warpage, 30% glass filled, pigmented black, injection molding PBT for industrial parts, rigid tough and dimensional stable.. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Comtuf® 420 Polyester - PBT, High Impact Modified Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Comtuf® 461 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Comtuf® 651 Nylon 6, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 412 Polyester - PBT, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 419 Polyester - PBT, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 420 Polyester - PBT, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 431 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Hiloy® 614 Nylon 6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Hiloy® 616 Nylon 6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Voloy® 461 Glass Reinforced, PBT Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 195 - 225 °C | 383 - 437 °F | |
AIM 40In/60Pb Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled PBT Description: Is a PBT, easy-flowing injection-molding grades with 15% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers, cove.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® B 4406 G6 30% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® B 4406 PBT Description: Is a PBT, flame-retardant injection-molding grades, unreinforced for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and lighting compo.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so.. |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | |
A. Schulman ComAlloy Comtuf® 463 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® B 4300 M2 12.5% Mineral Filled PBT Description: Is a PBT-HI, mineral-reinforced, impact-modified injection-molding grade for rigid parts, for example automotive power door locks.Information provided by BASF |
|||
Melting Point | 210 - 225 °C | 410 - 437 °F | Average value: 223 °C Grade Count:15 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Melting Point | 220 - 225 °C | 428 - 437 °F | DSC; ISO 11357-3 |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |