Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 160 - 170 °C | 320 - 338 °F | ASTM D3418 |
NatureWorks® Ingeo™ 3801X Injection Grade PLA Ingeo™ 3801X is designed for injection molding applications that require high heat and high impact performance. This polymer grade has much more rapid crystallization kinetics than other NatureWork.. |
|||
Melting Point | 160 - 170 °C | 320 - 338 °F | ASTM D3418 |
NatureWorks® Ingeo™ 6201D Fiber Grade PLA NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically .. |
|||
Melting Point | 160 - 170 °C | 320 - 338 °F | ASTM D3418 |
NatureWorks® Ingeo™ 6202D Fiber Grade PLA NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically .. |
|||
Melting Point | 155 - 170 °C | 311 - 338 °F | ASTM D3418 |
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co.. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | Huntsman/TMA |
Huntsman IROGRAN® A 85 P 4394 TPU-Polyether Introduction: IROGRAN A 85 P 4394 is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 4394 is part of the HUNTS.. |
|||
Melting Point | 142 - 170 °C | 288 - 338 °F | 0.025" extruded film, |
Huntsman IROGRAN® PS442-202 TPU-Polyester Introduction: IROGRAN PS440-202 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN PS440-202 is part of the HUNTSMAN .. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 131 - 170 °C | 268 - 338 °F | |
Indium Corp. Indalloy 99 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 140 - 170 °C | 284 - 338 °F | |
LG Chemical SEETEC H5300 Polypropylene, Homopolymer Features: Seetec H5300 is designed for the extrusion of textile yarn and monofilaments. This grade is characterized by good processability and stretchability. SEETEC H5300 meets the FDA requirement .. |
|||
Melting Point | 140 - 170 °C | 284 - 338 °F | |
LG Chemical SEETEC H7411 Polypropylene, Homopolymer Features: Seetec H7411 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by high tenacity from narrow molecular weight distribution (MWD) and U.. |
|||
Melting Point | 140 - 170 °C | 284 - 338 °F | |
LG Chemical SEETEC H7600 Polypropylene, Homopolymer Features: Seetec H7600 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by medium MWD and good heat stability. SEETEC H7600 meets the FDA requ.. |
|||
Melting Point | 140 - 170 °C | 284 - 338 °F | |
LG Chemical SEETEC H7700 Polypropylene, Homopolymer Features: Seetec H7700 is designed for the extrusion of fine fibers with the spunbond technology. This grade is characterized by very narrow molecular weight distribution (MWD), with anti-gas fading.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC M1425 Polypropylene Impact Copolymer Features: SEETEC M1425 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1425 exhibits a very high stiffness and a good impact strength. SEETEC M1425 meets the FD.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer Features: SEETEC M1600 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1600 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC M1700 Polypropylene Impact Copolymer Features: SEETEC M1700 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1700 exhibits a very high flowability and a good balance of stiffness and impact strength.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC R1610 Polypropylene Random Copolymer Features: SEETEC R1610 is a highly transparent ethylene-propylene random copolymer for injection molding applications. SEETEC R1610 exhibits an excellent transparency and a good impact strength. SEE.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC R3400 Polypropylene Random Copolymer Features: Seetec R3400 is a polypropylene-ethylene random copolymer designed for non-transparent injection molding application. SEETEC R3400 meets the FDA requirement in the code of Federal Regulati.. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | |
LG Chemical SEETEC R3420 Polypropylene, Random Copolymer Features: Seetec R3420 is a polypropylene-ethylene random copolymer designed for the production of cast films. It has a good clarity due to the optimum content of ethylene and offers optimum balance.. |
|||
Melting Point | 138 - 170 °C | 280 - 338 °F | |
Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 164 - 170 °C | 327 - 338 °F | ISO 3146 |
Borealis Bormod™ HD915CF Polypropylene Homopolymer for Cast Film Bormod HD915CF is a high crystallinity homopolymer film resin, based on special Borstar nucleating technology, especially developed for the manufacturing of unoriented film for metallizing. It is s.. |
|||
Melting Point | 165 - 170 °C | 329 - 338 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® HP30 KG30 NL HS 0B PPCP, 30% glass fiber/glass bead reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Melting Point | 160 - 170 °C | 320 - 338 °F | |
BCC Products BC 100 Thin Cyanoacrylate Adhesive BC100 Thin is a low viscosity material ideal for bonding larger areas. BC100 Thin has a 20 second fixture cure and able to fill gaps of .002” wide. BC100 Thin is perfectly designed for bonding plas.. |
|||
Melting Point | 138 - 170 °C | 280 - 338 °F | |
AIM 54Sn/26Pb/20In Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 130 - 170 °C | 266 - 338 °F | Average value: 162 °C Grade Count:52 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | Average value: 164 °C Grade Count:14 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Melting Point | 162 - 170 °C | 324 - 338 °F | Average value: 166 °C Grade Count:38 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Melting Point | 136 - 170 °C | 277 - 338 °F | Average value: 160 °C Grade Count:13 |
Overview of materials for Polypropylene with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in.. |