| Category | Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy |
| Manufacturer | Indium Corporation of America |
| Trade Name | Indalloy |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Indium Corp. Indalloy 281-338 Bismuth-Tin Solder Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 8.12 g/cc | 0.293 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Brinell | 23.5 <br>@Load 4.00 kg |
23.5 <br>@Load 8.82 lb |
2mm ball |
| Tensile Strength at Break | 51.7 MPa | 7500 psi | |
| Elongation at Break | 35 % | 35 % |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Heat of Fusion | 44.4 J/g | 19.1 BTU/lb | |
| Specific Heat Capacity | 0.180 J/g-°C | 0.0430 BTU/lb-°F | Solid |
| 0.213 J/g-°C | 0.0509 BTU/lb-°F | Liquid | |
| Thermal Conductivity | 30.0 W/m-K <br>@Temperature 85.0 °C |
208 BTU-in/hr-ft²-°F <br>@Temperature 185 °F |
|
| Melting Point | 138 - 170 °C | 280 - 338 °F | |
| Solidus | 138 °C | 280 °F | |
| Liquidus | 170 °C | 338 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Bismuth, Bi | 40 % | 40 % | |
| Tin, Sn | 60 % | 60 % |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Electrical Resistivity | 0.0000340 ohm-cm | 0.0000340 ohm-cm |