Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 295 °C | 563 °F | |
Techmer ES HiFill® PA4/6 GF25 HS NAT 25% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: Natural ColorInformation p.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® 46HF4530 PA46-GF30 30% Glass Reinforced, Heat Stabilized, High Flow, for E&E applications |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® 46HF5050 Nylon 46-50% Glass Reinforced (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
DSM Stanyl® TE250F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TS250F8 PA46-GF40 FR 40% Glass Reinforced, Flame Retardant, Heat Stabilized |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TS272A1 PA46-RF Aramid fiber reinforced, Wear and Friction Modified |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TS350 PA46 FR(17) Unreinforced, Flame Retardant |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | (DAM); ISO 11357-1/-3 |
DSM Stanyl® TW241F10 (COND) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TW241F3 Nylon 46-15% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Dry) Stanyl is a high performance polyamide providing performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temperature.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TW241F6 Nylon 46-30% Glass Reinforced, Heat Stabilized, Lubricated (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TW271B6 (PA46+PTFE)-CF30 30% Carbon Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
DSM Stanyl® TW271F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, PTFE Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | ISO 11357-1/-3 |
DSM Stanyl® TW300 (DAM) Nylon 46 Heat Stabilized, Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TW363 Nylon 46 (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® HT3Z black 9564 PA* Product description: Grivory HT3Z is an unreinforced and impact resistant, engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT product is partially ba.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4065 black 9238 PA*-GF50 Product description: Grivory XE 4065 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4134 black 9225 PA*-GF30 Product description: Grivory XE 4134 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53 736 |
Hippe PA 46 Nylon 46 PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4355 G5 BK 00564 25% Glass Filled PA6/6T (Conditioned) Description: 25% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Melting Point | 295 °C | 563 °F | DIN 53765 |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Dry) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Melting Point | 295 °C | 563 °F | 10°C/min; ISO 11357-1/-3 |
DSM Stanyl® TQ261F6 PA46-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Melting Point | 295 °C | 563 °F | 10°C/min (DAM); ISO 11357-1/-3 |
DSM Stanyl® TS256F6 Nylon 46-30% Glass Reinforced (Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |