Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1260 °C | 2300 °F | |
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std All values may vary dependent on specific design and usageAlumel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsulatedPlatedInformation provided by Californ.. |
|||
Melting Point | 1260 - 1357 °C | 2300 - 2475 °F | |
Kennametal Stellite Stellite® 6 PM cast Adhesive wear test data: 0.49 P/M, 0.48 Cast; Typical applications include: (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) die.. |
|||
Melting Point | 1260 - 1357 °C | 2300 - 2475 °F | |
Kennametal Stellite Stellite® 6 PM with P/M Processing Adhesive wear test data: 0.49 P/M, 0.48 Cast; Typical applications include: (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) die.. |
|||
Melting Point | 1260 °C | 2300 °F | |
Mid-Mountain Materials SILTEX® 1800 Amorphous Silica Industrial Textile SILTEX® 1800 is a family of high performance textiles comprised of high purity, high strength amorphous silica fibers. SILTEX® 1800 Industrial Textiles demonstrate excellent thermal stability,.. |
|||
Melting Point | 1260 - 1355 °C | 2300 - 2471 °F | |
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 0% Cold Worked, Not Aged 0% Cold Worked, Not Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes .. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 10% Cold Worked 10% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 15% Cold Worked, Aged 15% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 20% Cold Worked 20% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Melting Point | 1260 - 1355 °C | 2300 - 2471 °F | |
HP Alloys Alloy X, 30% Cold Worked 30% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International. |
|||
Melting Point | 1260 - 1335 °C | 2300 - 2435 °F | |
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Heat capacity, melting range, moduli, and Poisson's ratio re.. |
|||
Melting Point | 1260 - 1335 °C | 2300 - 2435 °F | |
Special Metals INCONEL® 718SPF™ Nickel Superalloy, Annealed + Aged Typical annealing - continuous process anneal, 1700°F (927°C) at 15 ft (4.57 m) per minute. This produces ASTM No. 12 grain size. Typical aging - 1750°F (954°C)/1 h/AC plus 1325°F (.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
Special Metals INCONEL® Alloy 718 Developed in the early 1960's, IN718 is still considered the material of choice for the majority of aircraft engine components with service temperatures below 1200°F (650°C). Inconel 718 is a.. |
|||
Melting Point | 1260 - 1340 °C | 2300 - 2440 °F | |
Special Metals INCONEL® Alloy G-3 A nickel-chromium-iron alloy with additions of molybdenum and copper. It has good weldability and resistance to intergranular corrosion in the welded condition. The low carbon content helps preven.. |
|||
Melting Point | 1260 - 1355 °C | 2300 - 2471 °F | |
Special Metals INCONEL® HX Nickel Superalloy Data provided by the manufacturer, Special Metals. |
|||
Melting Point | 1260 - 1405 °C | 2300 - 2561 °F | |
Special Metals UDIMET® alloy 520 Superalloy UDIMET® alloy 520 is a precipitation-hardenable nickel base superalloy with an exceptional combination of high-temperature mechanical properties, corrosion resistance and forgeability characteris.. |
|||
Melting Point | 1260 °C | 2300 °F | |
Unifrax FyreWrap® Marine Blanket Insulation FyreWrap® Marine Blanket from Unifrax is a totally inorganic, flexible, high-temperature insulation blanket specifically designed to provide passive fire protection for marine applications. The ca.. |
|||
Melting Point | 1260 - 1355 °C | 2300 - 2471 °F | |
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening.. |
|||
Melting Point | 1260 - 1343 °C | 2300 - 2449 °F | |
ATI Allvac® 718Plus™ Nickel Superalloy Allvac 718Plus alloy (UNS N07818) is a precipitation hardened nickel-base material that exhibits high temperature tensile strength and stress rupture performance. This alloy is designed to have the.. |
|||
Melting Point | 1260 °C | 2300 °F | |
Universal Wire Works No. 12 Cobalt Alloy Welding Wire Universal No. 12 is a cobalt-chromium-tungsten alloy suited for applications requiring extreme abrasion and corrosion resistance with moderate impact. The deposited hardness range of Rc 48 - 52 rema.. |
|||
Melting Point | <= 1260 °C | <= 2300 °F | |
Weartech International WT-20 Cobalt Hardfacing & Wear Resistant Alloy Applications: marine engine valves, control valves for petrochemicals, steel mill rolls, homogenizer valve componentsInformation provided by Weartech International |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 10% Cold Worked, Aged 10% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 15% Cold Worked 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 5% Cold Worked 5% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internatio.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 5% Cold Worked, Aged 5% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Inte.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 50% Cold Worked, Aged 50% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Melting Point | 1260 - 1355 °C | 2300 - 2471 °F | |
Special Metals INCONEL® Alloy HX A nickel-chromium-iron-molybdenum alloy with outstanding strength and oxidation resistance at temperatures to 2200°F (1200°C). Matrix stiffening provided by the molybdenum content results in high.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 20% Cold Worked, Aged 20% Cold Worked, Aged applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Int.. |
|||
Melting Point | 1260 - 1336 °C | 2300 - 2437 °F | |
HP Alloys Alloy 718, 25% Cold Worked 25% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, Inco Alloys International, and Haynes Internati.. |
|||
Melting Point | 1260 - 1355 °C | 2300 - 2471 °F | |
HP Alloys Alloy X, 15% Cold Worked 15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International. |