Material Notes:
15% Cold Worked applies to tensile and/or hardness; other properties are typical of this alloy.Data provided by High Performance Alloys, Inc., Allvac, and Haynes International.
Physical Properties Metric English Comments
Density 8.22 g/cc
0.297 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 945 MPa
137000 psi
Tensile Strength, Yield 731 MPa
106000 psi
Elongation at Break 20 %
20 %
Modulus of Elasticity 205 GPa
29700 ksi
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature 20.0 - 500 °C
8.33 µin/in-°F

@Temperature 68.0 - 932 °F
16.6 µm/m-°C

@Temperature 20.0 - 1000 °C
9.22 µin/in-°F

@Temperature 68.0 - 1830 °F
Thermal Conductivity 16.9 W/m-K

@Temperature 400 °C
117 BTU-in/hr-ft²-°F

@Temperature 752 °F
Melting Point 1260 - 1355 °C
2300 - 2471 °F
Solidus 1260 °C
2300 °F
Liquidus 1355 °C
2471 °F
Component Elements Properties Metric English Comments
Boron, B <= 0.0080 %
<= 0.0080 %
Carbon, C 0.10 %
0.10 %
Chromium, Cr 22 %
22 %
Cobalt, Co 1.5 %
1.5 %
Iron, Fe 18 %
18 %
Manganese, Mn <= 1.0 %
<= 1.0 %
Molybdenum, Mo 9.0 %
9.0 %
Nickel, Ni 47 %
47 %
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W 0.60 %
0.60 %