Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 123 °C | 253 °F | Internal method |
Polimeri Europa Clearflex® FG 308 Octene Copolymer Linear Low Density Polyethylene Clearflex FG 308 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 308 ar.. |
|||
Melting Point | 123 °C | 253 °F | Internal method |
Polimeri Europa Clearflex® FG 368 Octene Comonomer Linear Low Density Polyethylene Clearflex FG 368 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidant and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FG 368 ar.. |
|||
Melting Point | 123 °C | 253 °F | Internal method |
Polimeri Europa Flexirene® FG 23 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 23 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 U represents the version of Flexirene FG 20 U.. |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1002.32 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1002x74 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1002x79 Blown Film Resin
(discontinued **) LL1002 resins are butene LLDPE designed for blown film process, with good tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 5202.09 Compounding Resin
(discontinued **) LL 5202.09 is a linear low density polyethylene resin designed to provide good processability and ease of blending. The granular form of LL 5202.09 makes for efficient blending with pigments, slip .. |
|||
Melting Point | 123 °C | 253 °F | ASTM D3418 |
ExxonMobil LL 6202 Injection Molding Resin
(discontinued **) LL 6202 is a narrow molecular weight butene copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that require outstanding tear.. |
|||
Melting Point | 123 °C | 253 °F | Exxon Method |
ExxonMobil Escorene® LL-1117 LLDPE Film/Sandwich Bag Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE blown film resin. Films made from LL-1117 have very good tensile properties and toughness. This resin's good strength and drawability all.. |
|||
Melting Point | 123 °C | 253 °F | Eutectic |
Indium Corp. Indalloy 253 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 123 °C | 253 °F | ISO 11357 |
Total Lumicene® mPE M 3581 UV Metallocene Polyethylene, Rotomolding Lumicene® mPE M 3581 UV is a second generation metallocene medium density polyethylene with hexene as comonomer.Lumicene® mPE M 3581 UV is intended for the manufacture of rotomolded items.Its spec.. |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1002.09 Blown Film Resin Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat.. |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1107x93 Blown Film Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 1107x95 Blown Film Resin Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr.. |
|||
Melting Point | 123 °C | 253 °F | ASTM D3418 |
ExxonMobil LL 6201.19 Injection Molding Resin Product Description: LL 6201 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Melting Point | 123 °C | 253 °F | ASTM D3418 |
ExxonMobil LL 6202.19 Injection Molding Resin Product Description: LL 6202 is a narrow molecular weight butane copolymer designed for applications that require excellent toughness. This resin offers easy processability for applications that req.. |
|||
Melting Point | 123 °C | 253 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil NTX™ NTX 101 Super Strength Film Resin NTX 101 is a super strength hexene copolymer LLDPE film resin. Films made from this resin have outstanding toughness properties, especially impact and tear strength, compared to other hexene copoly.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow ATTANE™ 4201G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow ATTANE™ 4201G, 2mil Ultra Low Density Ethylene/Octene Copolymer ATTANE™ 4201G is used for packaging applications. It offers toughness, seal properties, optical properties and processability. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information prov.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7144 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as large industrial containers and trash cans. Information provide.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-8320 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in general purpose injection molding applications. Information provided by Dow |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DOWLEX™ 2070G Linear Low Density Polyethylene High strength in food packaging applications Good processability at narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DOWLEX™ 2077G Linear Low Density Polyethylene Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow DOWLEX™ 2077G Linear Low Density Polyethylene Fast processing on narrow die gaps Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a Information provided by Dow |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow ELITE™ 5401G Enhanced Polyethylene Resin ™ 5401G is a copolymer produced via INSITE™ Technology from Dow Plastics. It offers a unique combination of low seal initiation, moderate stiffness and low blocking for excellent performance on a.. |
|||
Melting Point | 123 °C | 253 °F | Dow Method (DSC) |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Melting Point | 123 - 129 °C | 253 - 264 °F | Average value: 127 °C Grade Count:8 |
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu.. |