Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 115 °C | 239 °F | Internal method |
Polimeri Europa Clearflex® CH D0 Very Low Density Polyethylene Clearflex CH D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The film has a high stretchability and an optimum cling effect.Main Applications:.. |
|||
Melting Point | 115 °C | 239 °F | Internal method |
Polimeri Europa Flexirene® MS 20 A Linear Low Density Polyethylene Flexirene MS 20 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 20 A are characterized by optimum low tempe.. |
|||
Melting Point | 115 °C | 239 °F | Internal method |
Polimeri Europa Flexirene® MS 26 A Linear Low Density Polyethylene Flexirene MS 26 A is a linear low density polyethylene (LLDPE), with antioxidants, suitable for injection molding application.Parts made with Flexirene MS 26 A are characterized by optimum low tempe.. |
|||
Melting Point | 115 °C | 239 °F | Internal method |
Polimeri Europa Riblene® BD 30 Low Density Polyethylene - Blow Molding Riblene BD 30 is a low density polyethylene resin (LDPE) characterized by high melt strength and optimum processability.Parts manufactured with Riblene BD 30 have good mechanical performances.Main A.. |
|||
Melting Point | 115 °C | 239 °F | Exxon Method |
ExxonMobil Exceed™ 363C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 363C32 resin have outstanding tensile properties and.. |
|||
Melting Point | 115 - 257 °C | 239 - 495 °F | ASTM D3418 |
3M Dyneon™ THV™ 200G Fluorothermoplastic, Pellet Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Melting Point | 115 - 160 °C | 239 - 320 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 85 E 4719 TPU-Polyester Introduction: IROGRAN A 85 E 4719 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offers a.. |
|||
Melting Point | 115 - 160 °C | 239 - 320 °F | 0.025" extruded film, |
Huntsman IROGRAN® A 85 E 5719 FCM TPU-Polyester Introduction: IROGRAN A 85 E 5719 FCM is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion and injection molding product range and offe.. |
|||
Melting Point | 115 - 150 °C | 239 - 302 °F | |
M Chemical GUARD DOGâ„¢ UV119 HALS Light Stabilizer GUARD DOGâ„¢ UV119 is effective in polypropylene, polyethylene, alpha-olefin copolymers and blends with EPR, ERR, PE, EVA, EAA, EVOH and filled PP.Typical Properties:Appearance - White to light y.. |
|||
Melting Point | 115 °C | 239 °F | TMA; MCI Method |
Mitsui APELâ„¢ APL6011T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melting Point | >= 115 °C | >= 239 °F | ISO 11357/03 |
Borealis Himod™ FT5270 LDPE for Film Himod FT5270 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Melting Point | 115 °C | 239 °F | Freezing point via DSC/ASTM D3418 |
DuPont Bynel® 4164 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 115 - 125 °C | 239 - 257 °F | DSC |
EMS-Griltech Griltex® D 1566A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 115 - 120 °C | 239 - 248 °F | DSC |
EMS-Griltech Griltex® D 1619E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 115 °C | 239 °F | Dow Method (DSC) |
Dow FLEXOMER™ GERS-1088 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ GERS-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to.. |
|||
Melting Point | 115 °C | 239 °F | Dow Method |
Dow AMPLIFY™ GR 209 Maleic anhydride grafted (MAH) polymer AMPLIFY™ GR 209 Functional Polymer is a post reactor maliec anhydride grafted (MAH) polymer. The base polymer is an ethylene-butene copolymer exhibiting high flexibility and elasticity. It can be.. |
|||
Melting Point | 115 - 120 °C | 239 - 248 °F | Optical birefringence |
Arkema Group PLATAMID® H106 PA80 Powder Copolyamide Platamid® H106 PA powder is a special purpose, medium melting point, very low viscosity, thermoplastic copolyamide adhesive suitable for thermal bonding and laminating of textile and foam substrate.. |
|||
Melting Point | 115 °C | 239 °F | Recrystallizing temperature; ISO 3146 |
Azdel Plus C200B01N 20% Chopped Fiber Mat / PP Resin Matrix AZDEL® C200B01 is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a v.. |
|||
Melting Point | 115 °C | 239 °F | Recrystallizing temperature; ISO 3146 |
Azdel Plus C321B02N 32% Chopped Fiber Mat / PP Resin Matrix AZDEL® C321B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Melting Point | 115 °C | 239 °F | Recrystallizing temperature; ISO 3146 |
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia.. |
|||
Melting Point | 115 °C | 239 °F | ASTM D4591 |
3M Dyneon™ THV 221GZ Fluoroplastic Granules 3M™ Dyneon™ Fluoroplastic Granules THV 221GZ is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of pellets. It provi.. |
|||
Melting Point | 115 °C | 239 °F | Recrystallizing temperature; ISO 3146 |
Azdel Plus C220B02N 22% Chopped Fiber Mat / PP Resin Matrix AZDEL® C220B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Melting Point | 115 °C | 239 °F | Recrystallizing temperature; ISO 3146 |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Melting Point | 115 °C | 239 °F | ASTM D4591 |
3M Dyneon™ THV 221AZ Fluoroplastic Agglomerate 3M™ Dyneon™ Fluoroplastic Agglomerate THV 221AZ is a flexible, transparent fluoroplastic composed of tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride in the form of agglomerate or.. |
|||
Melting Point | 115 °C | 239 °F | DSC |
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound with good low temperature properties and cut resistanceUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant properti.. |