Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 9.00 µm/m-°C
5.00 µin/in-°F
Below Tg; ISO 11359
Victrex® WG101™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, black, granules for injection moulding, easy flow with wear additivesWG101 does not contai..
CTE, linear, Parallel to Flow 9.00 µm/m-°C
5.00 µin/in-°F
Below Tg; ISO 11359
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
CTE, linear, Parallel to Flow 9.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
5.00 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RCL34 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 9.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
5.00 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP STAT-KON SE003 PA 12 (Europe-Africa-Middle East)
LNP* Stat-kon* SE003 is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Parallel to Flow 9.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
5.00 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP DC004E PC (Europe-Africa-Middle East)
LNP* Thermocomp* DC004E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding.
CTE, linear, Parallel to Flow 9.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
5.00 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP LX03447 PEEK
LNP* THERMOCOMP* LX03447 is a compound based on Polyetheretherketone containing Proprietary Filler(s).
CTE, linear, Parallel to Flow 9.00 - 15.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
5.00 - 8.33 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® B 6550 LN PBT
Description: High-viscosity grades for the extrusion of loose buffer tubes for optical fibers, semi-finished products for machining, profiles and pipes.Information provided by BASF