Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
PolyOne Trilliant™ HC X THC 1100 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® RCY6013 PC+ABS (Asia Pacific) Cycoloy* RCY6013 resin is an injection moldable high flow PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 V0 @ 1.5 mm.. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® RCY6113 PC+ABS (Asia Pacific) Cycoloy* RCY6113 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 5VB rating @ 2.0mm an.. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -40.0 - 60.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 140 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® RCY6214 PC+ABS (Asia Pacific) Cycoloy* RCY6214 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1.5 mm. D.. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
PolyOne Edgetek® XT X XT 1000 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP COLORCOMP D10006U PC LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP DBL34E PC (Europe-Africa-Middle East) LNP* LUBRICOMP DBL34E is a compound based on Polycarbonate resin containing Glass Bead, PTFE. Added features include: Easy Molding, Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC LNP LUBRICOMP* DL0029E is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Lexan® FXD164R PC (Europe-Africa-Middle East) Transparent/translucent medium viscosity PC for light diffusion special effects, FDA compliant and mold release containing. The color package may affect performance.This data was supplied by SABIC-I.. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C | 39.4 µin/in-°F | ISO 11359-1/-2 |
Lanxess Durethan® DP 2802/30 000000 Nylon 66, 30% Glass Fiber PA 66 injection molding grade, 30% glass fibers, UL 94V-2 at 0.75 mm , GWFI:960°C at 0.75 mm, GWIT: 775°C at 0,75 mm, halogen-freeApplication Examples: mixer insert for blenders, washing machi.. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RBG16I PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RBG16I is a compound based on Nylon 66 resin containing Glass Bead, Graphite. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DX12411C PC LNP* STAT-KON* DX12411C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP KF005 Acetal Copolymer LNP THERMOCOMP* KF005 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber. Added features of this material include: Chemically Coupled. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
ISO data |
Styron Magnum™ 555 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP D7001IXH PC LNP* THERMOCOMP* D7001IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare ap.. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
39.4 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP NX11302 PC+ABS (Asia Pacific) This is a PC/ABS compound with colorable, good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature 20.0 °C |
39.4 µin/in-°F @Temperature 68.0 °F |
ISO data |
Styron Magnum™ 213 ABS, General Purpose MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
39.4 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp WB008 PBT LNP* Thermocomp* WB008 is a compound based on Thermoplastic Polyester (PBT) containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
CTE, linear, Parallel to Flow | 71.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
39.4 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |