Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 48.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
26.7 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Cycoloy® CM5820 PC+ABS (Asia Pacific) Cycoloy CM5820 resin is a Mineral Filled Non-FR PC+ABS blend with high impact, high modulus, good chemical resistance & improved surface aesthetic, designed for hand help device chassis that require.. |
|||
CTE, linear, Parallel to Flow | 48.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP EL002 PEI LNP* Lubricomp* EL002 is a compound based on Polyetherimide resin containing 10% PTFE. Added features of this material include: Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 48.0 µm/m-°C @Temperature -30.0 - 100 °C |
26.7 µin/in-°F @Temperature -22.0 - 212 °F |
ISO 11359-2 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1040 PP SABIC® PPcompound 19T1040 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding application.. |
|||
CTE, linear, Parallel to Flow | 48.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
26.7 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-LOY AF3029U ABS (Europe-Africa-Middle East) LNP* STAT-LOY* AF3029U is a compound based on Acrylonitrile Butadiene resin containing Glass Fiber, Flame Retardant, Propietary filler. Added features include: Antistatic, UV-Stabilized. |
|||
CTE, linear, Parallel to Flow | 48.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66 LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
CTE, linear, Parallel to Flow | 48.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
26.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers. |
|||
CTE, linear, Parallel to Flow | 48.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
26.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
CTE, linear, Parallel to Flow | 48.0 µm/m-°C | 26.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM Stanyl® TC154 PA46 FR(17) Thermal conductive material, Flame Retardant, Heat Stabilized |
|||
CTE, linear, Parallel to Flow | 48.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
26.7 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR410 MT Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
CTE, linear, Parallel to Flow | 48.0 µm/m-°C | 26.7 µin/in-°F | dry; ISO 11359-1/-2 |
DSM EcoPaXX® Q-HGM24 PA410-(GF+MD)30 10% Glass Reinforced, 20% Mineral Reinforced, Heat Stabilized |