Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® 503R PC 10% GR PC. Optimum combination of high modulus plus excellent impact strength and flame retardance. UV-stabilized. Internal mold release. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL910 PC Various weight reductions at 0.250"" (6.35 mm) wall, 10% GR. High flexural strength and modulus, impact/heat resistant. V-0/5V at 0.250"" (6.35 mm). |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 95.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® FL410 PC Various weight reductions at 0.250: (6.38 mm) wall. Thin wall capability high flexural mod, strength and creep resistant. V-0/5V - 0.157""(3.98 mm). |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 2100F PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact Compliant, NSF 51 listing. WRAS certification in recognized col.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2100N PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -20.0 - 150 °C |
18.0 µin/in-°F @Temperature -4.00 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 2100N PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF13 HS L BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF13 X BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF14 HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Lubricated and Heat StabilizedAppearan.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF30 HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedProcessin.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF30 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 HR HS BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and Hydrolysis Resistant Appearance: .. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 HS L 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedProcessin.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PA6/6 GF33 UG BK 33% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF13 ML2 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and Molybdenum Disulfide Lubricant(2%)Features: Lubricated and Heat Stabiliz.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PA6/6 GF15 ML3 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: Molybdenum Disulfide LubricantFeatures: LubricatedAppearance: Natural ColorInformation provi.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PBT GB30 TL15 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Luriblend® PC GF10 TS15 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: PTFE + Silicone Lubricant(15%)Features: LubricatedAppearance: BlackInformation provided by T.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES Plastiblend® PPS/F 0328 Availability: North AmericaForms: Pellets Additive: Lubricant and Strontium Ferrite Features: LubricatedInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOTUF VF008 PA 66 (Asia Pacific) LNP THERMOTUF* VF008 is a compound based on Nylon resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PBT GF15 WT 096 LE 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: WhiteTPCI# 6862111Information provided by TP Composit.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PC GF10 UV BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAdditive: UV StabilizerAppearance: BlackInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Techmer ES HiFill® PES GM20 WT139 20% Milled Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Milled Glass Fiber, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C | 18.0 µin/in-°F | ASTM D696 |
Ensinger TECAPEI® 10% Glass Reinforced, made from Ultem® 2100 PEI TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in.. |
|||
CTE, linear, Parallel to Flow | 32.4 µm/m-°C @Temperature -40.0 - 40.0 °C |
18.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E831 |
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |