Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 1.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
0.556 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp DEL34 PC (Europe-Africa-Middle East) LNP* Lubricomp* DEL34 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP f.. |
|||
CTE, linear, Parallel to Flow | 1.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.556 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC LNP STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 5% PTFE. Added features of this material include: Easy Molding, Electrically Conductive, Wear Resistan.. |
|||
CTE, linear, Parallel to Flow | 1.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.556 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Stat-kon TE002 LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
CTE, linear, Parallel to Flow | 1.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.556 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON TE002 PU LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Parallel to Flow | 1.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
0.556 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP DC0049XF PC LNP* THERMOCOMP* DC0049XF is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant. |
|||
CTE, linear, Parallel to Flow | 1.00 - 5.00 µm/m-°C @Temperature 20.0 °C |
0.556 - 2.78 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,.. |