Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 84.0 µm/m-°C
46.7 µin/in-°F
ASTM D696
PolyOne Geon™ HTX Ultra LA426 Gray 2382 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
CTE, linear, Parallel to Flow 84.0 µm/m-°C
46.7 µin/in-°F
ASTM D696
PolyOne Geon™ HTX Ultra LA426G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Higher gloss version of Geon HTX Ultra LA426Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA426G Black 2880.Information provided by Pol..
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature 20.0 °C
46.7 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 105-28 Cellulose Acetate  (discontinued **)
28% Plasticized ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature 20.0 °C
46.7 µin/in-°F

@Temperature 68.0 °F
Eastman Tenite 132E-28 Cellulose Acetate  (discontinued **)
28% Plasticized with 25% fiber grade ester.ISO data as provided by the manufacturer, Eastman Chemical.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP
LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
46.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RP004 PA 66
LNP LUBRICOMP* RP004 is a compound based on Nylon 66 resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant.
CTE, linear, Parallel to Flow 84.0 µm/m-°C

@Temperature 20.0 °C
46.7 µin/in-°F

@Temperature 68.0 °F
ISO data
Styron Magnumâ„¢ SPD 214 ABS